Nondestructive Precious Metals Assay and Karat ID


Get fast, accurate analysis results with the GoldXpert Portable Benchtop XRF Analyzer

The GoldXpert XRF analyzer is an easy-to‑use, cost-effective method to obtain alloy chemistry and karat classification with one nondestructive and non-intrusive test. And, in an economic environment where fast and accurate results are more important than ever, the GoldXpert XRF analyzer provides outstanding precision and accuracy. Whether you buy gold, sell or produce jewelry, fabricate metal, or recycle scrap metal, you need a fast, highly accurate method to determine karatage (gold content) for quality control and pricing.

GoldXpert screen
XRF is a widely used, proven, and accepted method of chemistry analysis and karating of precious metals samples, including purity and fineness. XRF analysis provides a less expensive, quicker testing alternative to fire assay and chemical tests, and on-the-spot analysis of your silver, platinum, or other materials, making it an easy way to boost customer confidence and ensure dealer reliability.

GoldXpert

gold jewelry
On-the-spot gold karat classification, 0-24kt
diamond ring
Accurate compositional analysis of platinum, silver, and other precious metals
silver coin
Determination of Gold and Silver content in coinage
silver bracelet
Identify and analyze unknown metals for pricing, and even lead screening

Our analyzers give you the benefit and convenience of easy, on-the-spot analysis, so you can feel confident about the results for your gold and precious metal assets. The followed accuracy and precision data was generated using a GoldXpert with a Si PIN detector system, and is representative of typical performance expected from a Si PIN base system:

gold graph from GoldXpert
Results Graph from GoldXpert
Silver Results Graph from GoldXpert

GoldXpert Portable Benchtop XRF

The Compact Professional Precious Metals Testing Solution

The GoldXpert offers the best of both worlds. A handsome countertop analyzer fit for the consumer showroom environment, it can also be networked for high productivity QA/QC jobs. The large chamber door opens quickly, with a push of the large front trigger. The GoldXpert can also function as a portable analyzer, running off of a rechargeable Li ION battery pack. Compact and lightweight, weighing only 22 lbs (10 kg), the GoldXpert can be transported easily to wherever testing is needed.

Leaded glass viewing window - easily see sample in chamber

Integrated camera indicating sample analysis points

Safe-closed beam XRF system

Small spot collimation for analysis; ability to switch between 3-mm and 10-mm diameter spots with one push of a button

4 W X-Ray tube, 200 µA current (max) plus optimized beam settings for accurate analysis

Small desktop footprint: 267 mm x 310 mm x 340 mm (10.5 in. x 12.2 in. x 13.4 in.) (with door closed)

GoldXpert

LED-lit sample chamber: 125 mm x 210 mm x 180 mm (4.9 in. x 8.2 in. x 7.0 in.)

Analysis indicator light with 360° visibility

Portable - optional battery operation for mobile off-site use

USB interface for high-speed data export and printing

Responsive, bright, color touch screen display

Silicon PIN detector system standard. Silicon Drift Detector system available for optimized precision and sensitivity.

Olympus IMS
ProductsUsedApplications

The DELTA Element is a cost-effective handheld X-ray fluorescence (XRF) analyzer optimized for scrap metal sorting, positive material identification (PMI), alloy QA/QC, and precious metals analysis.
Combining a Silicon Drift Detector (SDD) and a 4W optimized X-ray tube, the DELTA Professional provides superior performance in speed, LODs, and elemental range. It analyzes Mg and higher for Alloys and Mining. The DELTA Professional is the best value solution from Olympus for handheld XRF.
The GoldXpert is a stylish countertop analyzer fit for the consumer showroom environment. Designed to be compact and lightweight, weighing only 22 lbs (10kg), the GoldXpert can be transported easily to wherever testing is needed. The GoldXpert gives accurate chemistry and karat results within seconds.
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.

This site uses cookies to enhance performance, analyze traffic, and for ads measurement purposes. If you do not change your web settings, cookies will continue to be used on this website. To learn more about how we use cookies on this website, and how you can restrict our use of cookies, please review our Cookie Policy.

OK