深穿透探头可与各种楔块配合使用,进行各种角度声束的检测应用。这些探头专用于深穿透应用,如对较厚平板、焊缝、锻件,及多噪声或晶粒状材料的检测。
A3, A4, and A5 probes
Deep penetration applications

| Part number | Frequency
(MHz) | Number of elements | Pitch
(mm) | Active
Aperture (mm) | Elevation(mm) | External dimensions
mm (in.) | ||
| L | W | H | ||||||
| 3.5L16-A3 | 3.5 | 16 | 1.60 | 25.6 | 16.0 | 36 (1.41) | 36 (1.41) | 25 (0.98) |
| 5L16-A3 | 5.0 | 16 | 1.20 | 19.2 | 12.0 | 36 (1.41) | 36 (1.41) | 25 (0.98) |
| 1.5L16-A4 | 1.5 | 16 | 2.80 | 44.8 | 26.0 | 57 (2.25) | 46 (1.80) | 30 (1.19) |
| 2.25L16-A4 | 2.25 | 16 | 2.00 | 32.0 | 20.0 | 57 (2.25) | 46 (1.80) | 30 (1.19) |
| 2.25L32-A5 | 2.25 | 32 | 0.75 | 24.0 | 24.0 | 29 (1.15) | 43 (1.67) | 24 (0.96) |
| 5L32-A5 | 5.0 | 32 | 0.60 | 19.2 | 20.0 | 29 (1.15) | 43 (1.67) | 24 (0.96) |
These probes come standard with an OmniScan® connector and a 2.5 m (8.2 ft) cable or can be specially fitted with other connectors and cable lengths. | ||||||||