Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds


Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds

Carbon Steel Weld Inspection

Magnetic particle inspection is used to help monitor the integrity of welded pipes and pressure vessels. This method was used for decades, primarily because of its portability and ease of use. It is a common industry practice to use specifically-designed oil and water-based carriers for magnetic particles, adding extra cost for chemicals and chemical waste disposal. In addition, this method also requires paint removal and repainting, adding additional cost to the inspection.

Eddy current inspection is an economical, nondestructive alternative to magnetic particle inspection. Eddy current inspection is fast, reliable, easy to use, and can inspect directly through painted surfaces. With eddy current, inspectors no longer have to strip and repaint pipes and vessels. As an added feature, eddy current makes it easy to record the defect length and depth.

Benefits of Eddy Current Array for Weld Inspection Compared to Magnetic Particle:

  • Eddy current array can be used through paint
  • Data can be recorded through paint
  • A welded part can be inspect using eddy current with lift-off compensation technology
  • Eddy current inspection is less impacted by weather
  • Intuitive, easy-to-understand imaging
  • Traceable results and post-process analysis
  • High scan speed and instant results
  • Quickly evaluate the depth of defects
  • Adjustable sensitivity

The inspection process using eddy current technology is fast, and the preparation is kept to a minimum—no intensive cleaning or paint removal is required. Eddy current inspection is also effective in most weather conditions including rain, heat, and cold. For easy post-processing analysis and data archiving, setup files can be saved and recalled for the next job. In addition, report files can be easily created directly from the instrument.

New Software Designed for Weld Applications

Eddy Current Array (ECA) Solution — OmniScan® Instruments

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 1: The Omniscan MX flaw detector with the MagnaFORM probe.

New ECA Probes Using Dynamic Lift-Off Compensation Technology

  • Robust ECA probe specially designed for weld applications
  • Flexible array probe helps ensure consistent contact with the weld
  • Dynamic lift-off compensation corrects sensitivity
  • Wear resistant probe protector, good for up to 22 km
  • Tool-free interchangeable wedges fit most pipes and vessels

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 2: The MagnaFORM probe.

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 3: The MagnaFORM probe unassembled.

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 4: The probe’s interchangeable wedges.

Ready for Scanners

  • Hand scanners, semi-automated scanners, and motorized scanners are available
  • Scanners suit pressure vessel and pipes

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 5: Image of MagnaFORM probe mounted on scanner

New Defect Depth Evaluation Tool

  • Quickly evaluate the size and depth of defects

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 6: A screen shot of the flaw detector’s measurement tools.

Reliable Defect Detection

The probe’s flexible PCB technology combined with dynamic lift-off compensation technology enables the solution to detect defects in all areas of the weld.

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 7: The defects located during a weld inspection.

Instant Reporting

The OmniScan MX flaw detector features built-in reporting at the touch of a key. Reports can also be configured and customized by advanced users.

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 8: An example of the first page of an OmniScan report.

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 9: The second page of an OmniScan report.

Easy Archiving

Archiving inspection data files is easy, simply press a key during acquisition or analysis to store the data on the instrument’s memory card.

Eddy Current as an Alternative to Magnetic Particle Inspection for Carbon Steel Welds
Figure 7: The defects located during a weld inspection.

Olympus IMS

应用所使用的产品
OmniScan X3系列的每台探伤仪都是一款功能齐备的相控阵工具箱。其创新型全聚焦方式(TFM)和高级相控阵(PA)功能助力您充满信心地识别缺陷,其性能强大的软件功能和便捷的工作流程有助于提高您的检测效率。
涡流阵列探头用于腐蚀探测、摩擦搅拌焊缝检测、表层和近表层缺陷检测。这种探头有助于加快检测的进程。
这款仪器可以进行涡流阵列检测。其检测配置支持32个传感器线圈(使用外置多路转换器可支持64个线圈),其工作模式可为桥式或发送接收式。其工作频率范围为20 Hz到6 MHz,并提供可以在同一采集操作过程中使用多个频率的选项。
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country