Ultra-Portable Rare Earth Element Exploration


An evolution of the DELTA Premium handheld XRF, the DELTA -50 offers a powerful 4 Watt, 50kV tube coupled with a large area, high resolution SDD. The DELTA -50 is ideal for rapid on-site compositional analysis of rock outcrop, soil, sediment, till, drill cuttings, diamond core and ore grade material. It is the optimal tool for on-site quantification of rare earth elements (REEs) including La, Ce, Pr, and Nd, as well as typical REE pathfinders including Y, Th, and Nb.

The real value arrives in the field where the Geoscientist can now use the realtime, "Instant Geochemistry" delivered by the DELTA to make decisions about site geology. Adapt sampling and mapping programs on-the-spot. Make immediate decisions while maximizing your exploration budget.

The DELTA-50 brings the power of a mobile lab to a handheld system - ruggedized and ultra portable. All DELTA XRF analyzers are engineered for continual use, carrying out thousands of tests per day in some applications, even in extreme environments. Engineered for rugged toughness AND analytical precision - there are no compromises!

Delta Handheld XRF Analyzer
Typical Limits of Detection (ppm)
Y 1-2
Th 2-3
Nb 2-3
Ag 3-5
Cd 2-3
Sn 5-8
Sb 5-7
Ba 20-25
La 30-50
Ce 45-60
Pr 65-100
Nd 75-350
Detection limits are a function of testing time, sample matrix and presence of interfering elements.
Detection limits are estimates based on 1-2 minutes test times and detection confidence of 3o (99.7% confidence).
Interference-free detection limits are intended as guidelines: please contact us discuss your specific application.

Data sample graphs

Olympus IMS

应用所使用的产品
DELTA Professional分析仪将硅漂移探测器(SDD)和一个4W优化X射线管结合在一起使用,可在检测速度、检出限及可检元素的范围方面提供非常高的性能。这款分析仪可以分析合金和矿石中镁(Mg)及原子数更高的元素。奥林巴斯所生产的DELTA Professional分析仪是一款性价比很高的手持式XRF分析仪。
在包含勘探、矿石品位/过程控制和保证环境可持续发展环节在内的整个矿产开发过程中,用于采矿和地球化学领域的DELTA手持式XRF分析仪可以即时得出检测结果,从而有助于决定所要采取的下一步措施。可在现场对金属、矿物及污染物进行探测。GPS-GIS-XRF用于即时绘制金属分布映射图,既节省时间又节省成本。
Sorry, this page is not available in your country
Let us know what you're looking for by filling out the form below.
Sorry, this page is not available in your country