Tube and Pipe Weld Inspection Using OmniScan™ PA

General Description of the Application

There are innumerable welded tubes and pipes in the oil and gas industry. From manufacture through the entire service life of these welded parts, they must be inspected and monitored because of pressure and toxic contents. Magnetic particle inspections are frequently used, but this technique is limited to surface or breaking defects. X-ray technique is also used, but is time consuming and requires a safety zone around the inspection area.

For these reasons, the use of ultrasonic inspections using the OmniScan™ Phased Array unit, manual scanner and 64-element probe provides major benefits: the most precise results, best images, fast inspections, and a nonhazardous inspection technique.

Typical Inspection Requirements
• Tube or pipe from 2 in. to 60 in. OD
• Wall thickness from 5 mm to 25 mm
• Portable equipment
• ASME Code compliant

Type of Defects
• Crack
• Lack of fusion
• Lack of penetration
• Porosity
• Undercut
• Slag inclusion

Description of the Solution
• Circumferential inspection using a manual scanner with one encoder
• Linear scanning around the weld. Electronic scanning at 60 degrees, then 70 degrees for each side of the weld.
• Imaging of real-time Top C-scan, Side B-scan, and Sectorial scan (S-scan)
• Primary analysis done with the OmniScan
• Postanalysis performed with TomoView® software

Advantages of the Solution
• High inspection speed
• Portability of the equipment
• Encoded linear scanning
• Electronic scanning from phased-array probe allowing accurate location characterization and sizing of defects



Equipment Required
OmniScan™ PA acquisition unit (Weld package)
• 5-MHz 64-element probe with 55-degree SW wedge
• Scanner
• Couplant system
TomoView™ software for advanced analysis

Inspection Method

Prior to any inspection conforming to the ASME code, a performance demonstration is required.

A zero-degree scan is performed on the near-weld material and the heat-affected zone (HAZ) to make sure the ultrasonic beam from the phased-array probe will penetrate the welded area properly. This scan is also used to find any laminations.

A first inspection is performed using a linear scan with an electronic scan using a 60-degree SW covering the complete volume of the weld. Then a second scan is made using a 70-degree SW. The same two angles are reused on the other side of the weld.

A first data analysis is made on the OmniScan™ after each scan. If an indication is found, the file is imported into TomoView™ where the indications are sized and characterized.

Products used for this application

OmniScan MX PA

OmniScan PA可进行手动和自动相控阵检测。这款仪器具有以下功能:全功能A扫描、B扫描、S扫描和C扫描显示,以及高级实时数据处理。可配置为16:128晶片、16:16M、16:64M、32:32和32:128。

OmniScan MX2NEW

具有触摸屏界面功能的OmniScan MX2相控阵探伤仪提高了检测效率,并具有强大的软件功能。使用这款仪器可以快速进行设置,缩短检测周期,并快速创建报告,从而保证了超水平的手动和高级AUT应用的特性。它与当前所有的相控阵模块都兼容。

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어