Curved array probes are made with a corrosion-resistant stainless steel case and are guaranteed waterproof up to 1 m underwater. The acoustic impedance of these probes matches water. They are compatible with adjustable immersion wedges and are used for the inspection of carbon fiber reinforced polymers (CFRP) corners and in addition to the inspection of composite for delamination.
| Part Number | Item Number | Casing Type | Frequency (MHz) | Number of Element | Pitch (mm) | Elevation (mm) | Radius (mm) (R) | Angle (°) (A) | Inspection Type |
| 3.5CC10.2-16-R1 | U8330453 | R1 | 3.5 | 16 | 1.0 | 5.0 | 10.2 | 90 | ID |
| 5CC10.2-16-R1 | U8330709 | R1 | 5.0 | 16 | 1.0 | 5.0 | 10.2 | 90 | ID |
| 3.5CC25-32-R4 | U8330629 | R4 | 3.5 | 32 | 1.32 | 6.0 | 25.0 | 90 | ID, OD |
| 5CC25-32-R4 | U8330479 | R4 | 5.0 | 32 | 1.32 | 6.0 | 25.0 | 90 | ID, OD |
| 3.5CC50-64-R5 | U8330630 | R5 | 3.5 | 64 | 1.65 | 6.0 | 50.0 | 121 | OD |
| 5CC50-64-R5 | U8330636 | R5 | 5.0 | 64 | 1.65 | 6.0 | 50.0 | 121 | OD |