Application: Measurement of individual layers and total thickness in coextruded plastic, both raw sheet stock and molded products.
As with any ultrasonic thickness measurement, accuracy is dependent on proper sound velocity calibration. Velocity calibration must be performed for each material being measured, on samples of known thickness. |