Measurement of wall thickness of steam boiler tubes with EMAT transducers

Recommended instruments:
Model 38DL PLUS thickness gage
Epoch XT, Epoch LTC, Epoch 1000, or EPOCH 600 flaw detector

Background: The very high temperatures found inside steam boilers (in excess of 1500 degrees Fahrenheit or 800 degrees Celsius) can cause the formation of a specific type of hard, brittle iron oxide called magnetite on the inside and outside surfaces of steel boiler tubing. The presence of this oxide layer on the outside of tubes can interfere with ultrasonic wall thickness measurement using common dual element transducers, both because it can have a very rough surface that prevents proper sound coupling, and because oxide thickness will be added to the steel thickness. However, as its name implies, magnetite is magnetic, and that property permits the use of magnetostrictive EMAT (Electomagnetic Acoustic Transducer) transducers such as the Panametrics-NDT E110-SB. EMATs offer several advantages over conventional dual element piezoelectric transducers: it is not necessary to remove oxide scale in order to make measurements, the scale thickness is not added into the wall thickness measurement, and measurements can be made very quickly and without need for liquid couplant. The primary limitation of magnetostructive EMATs is that they work only when scale is present and bonded to the outside of the boiler tube. Additionally, the minimum measurable wall thickness and measurement accuracy will not be nearly as good as what can be achieved with a conventional dual, and EMATs are relatively insensitive to small internal pits. For that reason, EMATs are often used for quick initial wall thickness surveys, while duals can then be used to take a closer look at areas of concern.

Theory of operation: There are two types of EMATs used within the NDT industry. One is known as a Lorentz EMAT, which does not require the presence of oxide scale, but does require very high driving power. A magnetostrictive EMAT such as the E110-SB requires scale but works at the much lower power levels typical of field portable ultrasonic gages and flaw detectors. It consists of a strong permanent magnet and a coil which acts as an electromagnet when driven by the excitation pulse from the test instrument, as seen in Figure 1. The permanent magnet creates a magnetic field perpendicular to the surface of the scale (Bs in the figure below), while the dynamic field created by the electromagnet (B d) causes the scale to be pulled radially outward and inward as the coil is pulsed, as seen in Figure 2. This motion generates a normal incidence shear wave in the scale, which then propagates into the steel. Essentially, the scale acts as the active transducer element to generate the sound pulse. The frequency of the sound pulse will vary as oxide thickness changes, increasing as oxide becomes thinner and decreasing as oxide becomes thicker. With typically thin scale buildups, the frequency will be approximately 5 MHz. The process also works in reverse to generate a voltage in the coil when the returning shear wave echo vibrates the scale.


Figure 1 -- Cross section of typical EMAT


Figure 2 -- Method of sound wave generation

Because the scale itself is the transducer element, scale roughness is not a coupling issue, and the scale is not added into the thickness measurement. The EMAT generates a shear wave, so the instrument must be calibrated to a shear wave velocity of approximately 0.1280 in/uS or 3,240 m/S in typical carbon steel. Typical measurement accuracy with the E110-SB EMAT transducer will be +/- 0.010 in. or 0.25 mm, with a minimum measurable thickness of at least 0.080 in. or 2.0 mm depending on material properties.

Setup and measurement procedures:As a general note, the quality of ultrasonic echoes in EMAT applications in part depends on the consistency of the oxide scale layer, which can vary from point to point on a given boiler tube. If usable echoes cannot be obtained at one point, try another point nearby. Also, the E110-SB transducer incorporates an adjustable standoff that varies the distance between the transducer face and the surface of the boiler tube. Adjusting this standoff distance will help optimize echo response in many cases.


(a) Model 38DL PLUS gage: The E110-SB transducer is used with the Model 38DL PLUS thickness gage in conjunction with a 1/2XA/E110 adapter, which provides both probe recognition and added high pass filtering that is necessary for proper signal conditioning. When the adapter is plugged in, the gage will automatically select the EMAT default setup DEFM1-EMAT/E110. As with any gage setup, for optimum accuracy a two-point velocity/zero calibration should be performed on thick and thin reference standards of known thickness, but if such standards are not available the default settings will usually be sufficient as a starting point. Instrument gain and echo blanking may be adjusted as necessary to optimize echo detection. Under the EMAT default setup, the 38DL PLUS will display a full wave rectified waveform. A typical waveform display is seen below in Figure 3.



Figure 3 -- Typical rectified EMAT waveform
For a more detailed look at the shape of the waveform, which can be useful under challenging measurement conditions, select the RF display more from the gage setup menu. A typical RF waveform from an EMAT measurement is seen in Figure 4.


Figure 4 -- Typical RF EMAT waveform


(b) EPOCH XT, EPOCH LTC, EPOCH 1000, or EPOCH 600: A typical EMAT starting setup and waveform for an Epoch series flaw detector is seen in Figure 5. Note that bandpass filtering must always be used to filter out low frequency noise associated with EMATs. Also, because shear wave frequency varies with oxide scale thickness, the Epoch's square wave frequency should be adjusted as necessary for optimum echo response.


Figure 5 -- Typical Epoch waveform and setup

Products used for this application

38DL PLUS

The 38DL PLUS is an advanced ultrasonic thickness gage. Uses dual element transducer for internally corroded applications, features include THRU-COAT and Echo-to-Echo. Uses single element transducers for very precise thickness measurements of thin, very thick, or multilayer materials.

EMAT Transducers

EMAT's are single element transducers that employ a magnetostrictive effect to transmit and receive ultrasonic waves.

EPOCH 1000 Series

The EPOCH 1000 is an advanced conventional ultrasonic flaw detector that can be upgraded with phased array imaging at an authorized Olympus service center. Key features include: EN12668-1 compliant, 37 digital receiver filter selections, and 6 kHz pulse repetition rate for high speed scanning.

EPOCH 600NEW

The EPOCH 600 is mid-level, handheld ultrasonic flaw detector. Weighing only 1.68 kg (3.72 lb.), its horizontal case is built to withstand the rigors of very harsh environments. EN12668-1 plus features such as 400 V PerfectSquare tunable square wave pulser, digital filtering for enhanced signal-to-noise ratio.

EPOCH LTC

The EPOCH LTC is a mid-level, handheld ultrasonic flaw detector in a compact 2.12 lbs (0.96 kg) vertical case. It is a full-featured instrument with EN12668-1 compliance and a wide variety of standard features as well as specialized options to meet your inspection needs.

EPOCH XT

The EPOCH XT is an advanced, portable ultrasonic flaw detector offering many standard measurement features including a tunable square wave pulser, selectable narrow-band and broad-band digital filters, gain range from 0 to 110 dB, peak memory and peak hold, and adjustable PRF.

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어