Several techniques can be used to eliminate or reduce the edge effect that affects or even prevents the inspection on areas close to edges, fastener heads, etc.

1. Shielding

Shielding is the most often used technique to avoid edge effect. Ferrite is the best material used and reduces the sensitive area to the
internal diameter of the shield. At lower frequencies the eddy currents will propagate slightly beyond the shield diameter.

2. Differential Coils

The use of differential coils can be helpful to avoid external interference such as edge effect. With the coils aligned to keep the same distance to the edge, it is possible to inspect sometimes even with an overlap.

3. Maintaining a Constant Distance

By using a guide it is possible to keep a constant distance to an edge or another object such as a fastener head (see Figure 1 and 2).

Figure 1

Figure 2



Figure 3

4. Using Directional Probes

Directional probes can be useful as their sensitivity at 90° is very low. The reflection sliding probes with transparent lenses are the best examples of this (see Figure 3). Because of low sensitivity at 90° they ignore edges and joints between two plates or skins. A straight edge can be useful as a guide (see Figure 4).



Figure 4

5. Using Directional Probes Across the Edge or Joint

The signal produced by the joint or edge can often be differentiated from the defect (see Figure 5).

Figure 5

6. Adding Another Piece of Similar Type Metal to Probe

By adding a piece of similar type metal to the probe, it is possible to establish a path for the eddy currents and sometimes use it as a guide as well (see Figure 6).

Figure 6

Products used for this application

Eddy Current Probes

Eddy current probes consist of the acquired brands of Nortec and NDT Engineering. We offer more than 10,000 standard and custom designed eddy current probes, standard references, and accessories.

Nortec 2000D

The Nortec 2000D+ eddy current flaw detector offers a frequency range of 50 Hz to 12 MHz, single or dual frequency operation, easy to use digital conductivity, and rotating scanner support making this flaw detector ideal for numerous aerospace applications.

Nortec 500

The lightweight Nortec 500 Series eddy current flaw detectors incorporate a full range of features such as internal balance coils and VGA output connector. Various models also include features such as conductivity and coating thickness, rotating scanner compatibility, and dual frequency.

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어