Inspection & Measurement Systems

Các sản phẩm cũ

1700

The Nortec® 1700 is designed for the customer that requires conductivity testing only.

Specifications:lawMaster™ is a Microsoft® Windows® 98/Me/NT/2000/XP program, which provides a user-friendly interface for communications between the flaw detector and an IBM compatible PC. A-Scans, instrument settings, thickness readings, and report contents are all available for review, archiving, uploading and downloading.

  • 60 or 480 KHz operation
  • 0.9 - 110% IACS
  • 0.0 - 0.025 inch non-conductive thickness readings
  • Large selection of probe configurations with reject LEDs
  • Fast, simplified sorting of metal alloys
  • Verification of aluminum heat treatment
  • Interchangeable probes require no factory calibration of instrument to probes

The Nortec® 1700 replaces the original Nortec® 17, once the standard in conductivity testing. Once setup is complete, alloys and heat-treated conditions or paint thickness can be checked automatically using the instrument's Go/No-Go alarm.

NORTEC® 1700 Technical Specifications
Conductivity Range: Digital conductivity display from 0.9% to 110% IACS. (International Annealed Copper Standard)

Accuracy: Within ± 0.5% IACS from 0.9% to 62% IACS and within ± 1% of values over 62%. Meets BAC 5651. Conductivity measurements with greater than 10 mils of lift-off have reduced accuracy.

Non-Conductive Coating Thickness: Can measure non-conductive coating thickness from 0.00" to 0.025". Accuracy of ± 0.001" over 0.00" to 0.015" range.

Alarms: Independent high and low limit alarms can be set for conductivity and lift-off. The alarms can be set to trigger when values are inside the limits (positive) or outside the limits (negative).

PowerLink™: Automatic probe recognition.

GENERAL
Dimensions: L = 9.5 in., W = 5.5 in., D = 3.5 in.; excluding handle (241 mm x 140 mm x 89 mm).
Weight: 6 lbs. (2.7 kg) with 2 Ni-MH batteries, 4.8 lbs. (2.1 kg) with 1 battery, 3.6 lbs. (1.6 kg) without batteries.
Display: Monochrome Backlit Liquid Crystal Display; 4.0 x 3.0 in. (5.0 in. diagonal), 320H x 240V pixels. Optional customer-interchangeable Hi-Brite Electroluminescent (EL) display.
Operating Temp: -4º to 140º F (-20º to 60º C).
Storage Temp: -40º to 176º F (-40º to 80º C).
POWER

DC: Two DR-35 Ni-MH batteries. Optional DR-35 battery pack or D-Cell belt pack.

AC: External charger eliminator will charge the internal battery and simultaneously operate a instrument from 90 to 264 volt, 50/60 Hz mains. Charging time is approximately 3 - 4 hours per battery pack.

Low Battery: Display bar graph "gas gauge" indicates approximate operating time. A low battery annunciator indicates when approximately 15 minutes of operation are left.

Battery Run Time: 8+ hours
Humidity: Safe operation in exposure to Class 3 temperature/humidity environment (-10° C to 55° C at 95% ± 5% relative humidity).

Hazardous Area Operation: Safe operation in explosive atmospheres as defined by Class 1, Division 2, Group D, as found in the National Fire Protection Association Code 0 (NFPA70), section 500 and tested using MIL-STD-810E, Method 511.3, procedure 1.


English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어