Inspection & Measurement Systems

Ультразвуковые приборы

OmniScan MX UT

OmniScan MX UT

The OmniScan MX UT performs conventional UT and automated inspections and supports TOFD as well as encoded B-scan and C-scan, and full data storage. Allows inspections that simultaneously combine TOFD with conventional pulse echo.

Ultrasound Inspection

Time-of-Flight Diffraction Testing

Time of Flight Diffraction Testing with OmniScan

Time-of-flight diffraction (TOFD) is a technique that uses two probes in pitch-catch mode. TOFD detects and records signals diffracted from defect tips allowing both detection and sizing. The TOFD data is displayed in a grayscale B-scan view. TOFD offers wide coverage and amplitude-independent sizing complying with the ASME‑2235 code.

  • One-line scan for full-volume inspection
  • Setup independent of weld configuration
  • Very sensitive to all kinds of defects and unaffected by defect orientation

TOFD and Pulse-Echo Testing

Time of Flight and Pulse-Echo diagram
Time of flight and Pulse-Echo diagram

While TOFD is a very powerful and efficient technique, its coverage is limited as a result of two inspection dead zones: one dead zone is near the surface, the other is at the backwall.

The OmniScan® UT allows inspections that simultaneously combine TOFD with conventional pulse echo. Pulse echo complements TOFD, covering the dead zones.

  • TOFD inspection
  • 45º pulse echo for weld cap inspection on either side of the weld
  • 60º pulse echo for weld root inspection on either side of the weld

0‑Degree Testing (Corrosion and Composite)

0-degree testing measures the time-of-flight and amplitude of ultrasonic echoes reflecting from the part into gates in order to detect and measure defects.

  • C‑scan imaging
  • Full A‑scan recording with C‑scan postprocessing

Ultrasound Software

Full-Featured C‑Scan

OmniScan MX UT C-Scan screen

  • Monitors amplitude, peak position, crossing level position, and thickness on each gate.
  • Automatic gate synchronizes from previous gate for higher dynamic range of thickness.
  • A‑scan data storage and C‑scan postprocessing capabilities
  • Optional IF gate for surface-following synchronization or measurement gate, or TCG/DAC curves
  • Positive or negative gate on RF signal (independent for each gate)
  • Eight completely configurable alarms on single-gate events or multiple-gate events, filter for n occurrences from one or multiple channels
  • Customizable color palette for amplitude and thickness C‑scans
  • Adjustable 256-level color palette
  • 2‑axis mechanical encoding with data-acquisition synchronization on mechanical movement
  • Optional data library to access A‑scans and/or C‑scans on PCs for custom processing

Full-Featured B‑Scan

  • Easy-to-interpret cross-sectional view of inspected part
  • Excellent display of corrosion mapping for boilers, pipes, and storage tanks
  • Visual identification of acquired thickness values
  • Encoded TOFD capability for amplitude-independant defect sizing

Full-Featured A‑Scan

A-Scan from OmniScan MX UTA-Scan Omniscan MX UT

  • Color‑selectable A‑scan display
  • Reject mode
  • Hollow mode
  • Peak-hold mode (always keeps the signal that shows the maximum amplitude in gate A)
  • Gate threshold-level crossing (changes the color of the curve that is over the gate level)
  • 60-Hz A‑scan refresh rate with overlays of envelope and peak inside the gate

Step-by-Step Calibration Wizards

All calibration procedures are guided using step-by-step wizards.

  • Sound velocity calibration
  • Wedge delay calibration
  • TOFD calibration
  • TCG calibration
  • Encoder calibration

TOFD Option

  • B-scan encoded data imaging and storage
  • Grayscale color palette, adjustable for brightness and contrast
  • 100-MHz A‑scan digitizing
  • TOFD calibration wizard, online and offline
  • Hyperbolic cursor and reading for TOFD sizing
  • Lateral wave resynchronization
General
Overall dimensions
(W x H x D)
244 mm x 182 mm x 57 mm
(9.6 in. x 7.1 in. x 2.1 in.)
Weight 1 kg (2.2 lb)
Connectors LEMO® 00 (2, 4, or 8)
Pulser
Number of pulsers 2, 4, or 8
Pulse output 50 V, 100 V, 200 V, 300 V ±10 %
(variable pulse width)
Pulse width Adjustable from 30 ns to 1000 ns ±10 %, resolution of 2.5 ns
Fall time Less than 7 ns
Pulse shape Negative square wave
Output impedance Less than 7 Ω
Receiver
Number of receivers 2, 4, or 8
Receiver gain range 0 dB to 100 dB, by steps of 0.1 dB
Maximum input signal 20 Vp-p (screen at 128 %)
Minimum sensitivity 200 µVp-p (screen at 128 %)
Noise referred to input 160 µVp-p (26 µV RMS) (128 %)
Input impedance 50 Ω
Input filter
(100 % bandwidth)
Centered at 1 MHz (1.5 MHz),
centered at 2 MHz (2.25 MHz),
centered at 5 MHz (4 MHz),
centered at 10 MHz (12 MHz),
centered at 15 MHz,
centered at 20 MHz;
0.25 MHz to 2.5 MHz, 2 MHz to 25 MHz BB
System bandwidth 0.25 MHz to 32 MHz (-3 dB)
Rectifier Both, positive, negative
Mode PE (pulse-echo), PC (pitch-catch), TT (through-transmission). In PC mode the maximum number of pulsers equals the number of channels divided by 2.
Smoothing Digital
DAC
Number of points 16
DAC range Up to 40 dB
Maximum gain slope 20 dB/µs
Data acquisition
A-scan acquisition rate 6000 A-scans/s (512-point A-scan)
Maximum pulsing rate 1 channel at 12 kHz (C-scan)
Data processing
Real-time averaging 2, 4, 8, 16
Gates
Quantity 3: I (synchro), A and B (measure)
Synchronization I, A, B referenced on main bang; A and B referenced on gate I (post-synchronization)
Data storage
A-scan recording (TOFD) 6000 A-scans/s (512-point A-scan)
(3 MB/s transfer rate)
C-scan type data recording 12 000 (A1, A2, A3, T1, T2, T3) (3 gates)
12 kHz
(lower frequency for corrosion mapping)
Data visualization
Refresh rate 60 Hz
Data synchronization
On time 1 Hz to 12 kHz
On encoder On 1 or 2 axes divided into 1 to 65 536 steps
Alarms
Number 3
Conditions Any logical combination of gates
Signal Amplitude or TOF of gate A or B

Inspector inspecting a large pip using the OmniScan MX UT

Introducing the OmniScan 2-channel UT B-Scan Corrosion Mapping Kit.

This kit includes the OmniScan MX UT, the manual Remote Scan B-scan position encoder, TomoView Lite software, and a dual-UT probe. This kit addresses your B-scan inspection needs-for spot checks and one-line scans on ferrous steel structures, plates, pipes, and more.

Remote Scan, B-scan position encoder OmniScan MX UT (2 channels) TomoView Lite for postprocessing

Loading...

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어