A 2-axis scanner for manual ultrasonic inspections. One scanning axis is flexible and conforms to the contour of the part being inspected. Vacuum cups make the Wing Scanner well suited for nonferromagnetic surface inspections.
The WING™ Scanner is a two-axis scanner for manual ultrasonic inspections. One scanning axis is flexible and conforms to the contour of the part being inspected. Vacuum cups make the WING Scanner well-suited for nonferromagnetic surface inspections.
Typical applications include the inspection of friction stir welding (FSW) and the inspection to detect delamination, cracks, and corrosion on plates and airplane fuselage.

Flexible X-axis
Rigid Y-axis
| Wing Scanner V1 | Wing Scanner V2 | Wing Scanner H1 | |
| X-axis stroke (mm) | 940 | 1940 | 940 |
| Y-axis stroke (mm) | 510 | 510 | 510 |
| Vaccum generation * | Venturi with air supply | Manually activated levers | |
| Minimum external radius (mm) | 360 | 380 | 450 |
| Minimum internal radius (mm) | 770 | 770 | 770 |
| Holding force (kg/cup) | 30 | 30 | 11 |
| Number of cups | 10 | 19 | 8 |
| Total weight (kg) | 6.3 | 8.8 | 7.0 |
| Overall scanner length (X-axis) (mm) | 1395 | 2395 | 1120 |
| Overall scanner length (Y-axis) (mm) | 790 | 790 | 790 |
| Total height (mm) | 157 | 157 | 165 |
|
* For "V" models, compressed air characteristics must correspond to the following specifications:
Required pressure: 490 kPa to 690 kPa (71 psi to 100 psi) Flow rate: 566 nl/min (20 SCFM) minimum | |||