高解像度渦流プローブは、コイルがプラスチック製スリーブで保護され、前部および後部がステンレス製の耐磨耗ガイドになっている頑丈かつ軽量なプローブです。巻きの狭いコイルのため、チタニウム製チューブなどの薄型チューブの検査に最適です。

Features

  • Narrow coil, ideal for thin tubing inspection such as titanium tubing.
  • Lightweight, solidly built.
  • Coils protected by a plastic sleeve.
  • Stainless steel wear guides at the front and rear ends.

Standard/Custom Probes (Made to Order)

Use the nomenclature and the chart below to configure your part number.

Probe Type Probe Diameter *
(use mm in part ID)
Center Frequency Cable Length
(TEK only)**
mm in.
TEK: Attached
TEL: Detachable
Use with TEZ-BBS or TEZ-BBK cables.**
Standard
TEK: 9.6 mm to 50 mm
TEL: 11 mm to 50 mm
by 0.2 mm
Custom (TEK only)
50.2 mm to 100 mm
Standard
TEK: 0.378 in. to 1.969 in.
TEL: 0.433 in. to 1.969 in.
by 0.008 in.
Custom (TEK only):
1.976 in. to 3.937 in.
015 (Low)
050 (Mid)
250 (High)
600 (Very High)
15 m (50 ft)
20 m (65 ft)
30 m (100 ft)
**TEZ cable information for TEL probes is available in the Tube Inspection Probe Catalog.