HSMT-X03スキャナーは、構造溶接部用スキャナーで、ほとんどのプローブが装着可能です。プローブホルダー(オプション)の使用でプローブを10個まで装着可能、外径38インチ(965 mm)以上のパイプの溶接部の全断面を検査できます。
The HSMT-X03 is the construction weld scanner offering the most probe-holding capacity. In fact, the scanner can hold up to 10 probes1 for either phased array or conventional UT, in order to obtain optimal coverage of the entire weld volume.
The basic configuation is intended for construction welding inspection. In order to be used in more restricted areas, the scanner can also be reconfigured with the provided short frame bars.
Note: Umbilical cable, probes, and wedges are not included with the scanner.
|
Length in Scan Axis
(mm) |
Width
(mm) |
Height
(mm) |
Weight
(kg) |
| 279 | 413 | 131 | 3.2 |