Industrial Testing Instruments

TOFD探触子

超音波装置

Our time-of-flight diffraction transducers are highly damped longitudinal wave probes that offer excellent resolution in challenging TOFD applications. These highly sensitive composite element broadband transducers are available in frequencies from 2.25 MHz to 15 MHz and in sizes from 3 mm (0.25") to 12 mm (0.50"). They are for use with specialized TOFD wedges designed to produce refracted longitudinal waves in steel.

Miniature Screw-in TOFD Transducers

Freq

Nominal Element Size

Transducer Part Numbers

Case
Type

Case Thread Pitch

MHz

inches

mm

2.25

0.25

6

C542-SM

ST1

3/8 - 32

0.375

9.5

C566-SM

ST2

11/16 - 24

0.5

12

C540-SM

ST2

11/16 - 24

5.0

0.125

3

C567-SM

ST1

3/8 - 32

0.25

6

C543-SM

ST1

3/8 - 32

0.375

9.5

C568-SM

ST2

11/16 - 24

0.5

12

C541-SM

ST2

11/16 - 24

10

0.125

3

C563-SM

ST1

3/8 - 32

0.25

6

C544-SM

ST1

3/8 - 32

15

0.125

3

V564-SM

ST1

3/8 - 32

Transducer Dimensions (in inches)

Case Type

(A)

(B)

(C)

Thread Pitch

ST1

0.44

0.55

0.22

3/8 - 32

ST2

0.71

0.685

0.257

11/16 - 24

Miniature TOFD Screw-in Wedges

ST1 Wedge Type

ST2 Wedge Type

Refracted Longitudinal Angle

Wedge Options

(°)

ST1-45L

ST2-45L

45

Standard

ST1-45L-IHC

ST2-45L-IHC

45

Irrigated*

ST1-60L

ST2-60L

60

Standard

ST1-60L-IHC

ST2-60L-IHC

60

Irrigated*

ST1-70L

ST2-70L

70

Standard

ST1-70L-IHC

ST2-70L-IHC

70

Irrigated*