
Sliding probes are specifically designed to inspect rows of fasteners. They operate in the reflection mode (Driver/Pickup coils) and are used to find surface and near-surface flaws. Available in two different types; adjustable types (as shown in picture below) include shims that allow the probe to be adjusted to accommodate different fastener sizes and include microdot connectors. Fixed types are capable of finding the same flaws as the adjustable but usually are procedure specific due to coil size and frequency range. The fixed versions typically include the Fischer/LEMO triax connector and the underside of the probe is relieved to allow the probe to easily slide over raised fastener heads.
Sliding probes are specifically designed to inspect rows of fasteners. They operate in the reflection mode (Driver/Pickup coils) and are used to find surface and near-surface flaws. Available in two different types; adjustable types (as shown in picture below) include shims that allow the probe to be adjusted to accommodate different fastener sizes and include microdot connectors. Fixed types are capable of finding the same flaws as the adjustable but usually are procedure specific due to coil size and frequency range. The fixed versions typically include the Fischer/LEMO triax connector and the underside of the probe is relieved to allow the probe to easily slide over raised fastener heads.
|
Dimensions
mm (in.) | |||||||
| Part Number | Item Number | Type | Frequency Range | Height | Length | Width | Connector |
| LTW0419-1 | U8633025 | Adjustable | 100 Hz to 5 kHz | 25.4 (1.00) | 85.1 (3.35) | 19.1 (0.75) | (2) 1-pin Microdot |
| LTW2018-1 | U8633056 | Adjustable | 500 Hz to 10 kHz | 25.4 (1.00) | 44.7 (1.76) | 25.4 (1.00) | (2) 1-pin Microdot |
| LTW0423-1 | U8690009 | Adjustable | 500 Hz to 10 kHz | 25.4 (1.00) | 44.5 (1.75) | 25.4 (1.00) | (2) 1-pin Microdot |
| LTW5010-1 | U8690010 | Adjustable | 1 kHz to 20 kHz | 25.4 (1.00) | 25.4 (1.00) | 25.4 (1.00) | (2) 1-pin Microdot |
| LTW1022 | U8633026 | Adjustable | 5 kHz to 100 kHz | 25.4 (1.00) | 38.1 (1.50) | 19.1 (0.75) | (2) 1-pin Microdot |
| NEC-4039 | U8636053 | Fixed | 1 kHz to 100 kHz | 25.4 (1.00) | 38.1 (1.50) | 20.3 (0.80) | Fischer/LEMO Triax |
| NEC-4039-1 | U8633054 | Fixed | 1 kHz to 100 kHz | 25.4 (1.00) | 38.1 (1.50) | 20.3 (0.80) | 2-pin Microdot |
| NEC-4039-2 | U8633055 | Fixed | 1 kHz to 100 kHz | 25.4 (1.00) | 38.1 (1.50) | 20.3 (0.80) | 4-pin Fischer |
| NEC-4039-3 | U8629545 | Fixed | 1 kHz to 100 kHz | 25.4 (1.00) | 38.1 (1.50) | 20.3 (0.80) | (2) 1-pin Microdot |
| NEC-4039-7L | U8633027 | Fixed | 1 kHz to 100 kHz | 38.1 (1.5) | 58.4 (2.3) | 30.4 (1.2) | 7-pin LEMO |
Copyright 2011 OLYMPUS CORPORATION, All rights reserved. |利用規約|個人情報保護方針/プライバシーポリシー
