PipeWIZARDを使用したパイプ溶接部自動超音波探傷検査

Meets or exceeds API 1104, DNV 2000, OS101, and ASTM E-1961 AUT codes

  • Proven and qualified AUT system for double and quadruple jointing at mill, as well as onshore and offshore pipeline construction
  • Safe system: no radiation hazard
  • Efficient system: no disruption of normal operation
  • Money-saving system: better process control of welding, giving lower reject rates
  • Better weld quality with unique system performance
  • High defect detection capability
  • Extra beams for key areas, such as root passes
  • Any weld profile: CRC-Evans, J-bevel, modified J-bevel, V,double V .
  • Better productivity
  • Wide range of pipe diameters and wall thicknesses
  • Fast scanning speed: 100 mm/s
  • Cycle time of approximately two minutes for 36-inch pipe welds
  • Rapid data interpretation (virtually in real-time)




PipeWIZARD phased-array automated ultrasonic inspection system (AUT).


Lack of fusion detection confirmed by macrophotography.


Ultrasonic zone discrimination is a key feature of AUT with PipeWIZARD.

System Description
  • Tomoscan FOCUS™ 32:128 phased-array unit
  • Motor drive unit
  • Industrial PC
  • Downsized probe pan containing two linear arrays
  • Mechanized drive clamping onto welding band
  • 25 m umbilical cable connecting probes, encoder, power, and couplant lines to instrumentation
  • Instrumentation console including PC, pulsers, and motor drive
  • Couplant containers, pump, and reclamation unit


Probe Pan Description
  • Probe pan contains two linear arrays.
  • Extra modules are available for transverse or dedicated TOFD inspections.
  • Couplant is pumped water or water-methanol in cold climates.
  • Encoder running on welding band gives circumferential position.

    Software Description
  • Custom PipeWIZARD™ software running on Microsoft® Windows NT® for data acquisition, analysis, and reporting
  • Automatic marking of indications exceeding rejection threshold to assist the operator
  • Inspection reports and list of defects adapted to client requirements
  • Automatic saving to two separate media in real time
  • Automated inspection sequence

PipeWIZARD

Pipe diameter 50 mm to 1424 mm (2 in. to 56 in.)
Pipe wall thickness 6 mm to 36 mm (0.25 in. to 1.5 in.) or more depending on wall thickness and addtional transducers. (Additional transducers may be required.)
Array Two linear 7.5-MHz, 60-element, 75 mm long
Scan speed 100 mm/s (4 in./s)
Scanner size 250 mm (L) x 120 mm (W) x 75 mm (H)
Scanner weight 2 kg (4 lb)
Additional probe pan slots Extra slots for eight conventional transducers for transverse defects or additional scans
Weld profile All common welds: CRC-Evans, J-bevel, manual, V, double V, X, etc. (any profile in principle)

Ultrasonics

Method Multichannel zone discrimination or custom scans as specified
Zone size <1 mm possible using increased number of zones.
(Maximum number of zones is 32 per view, and four views are available for a total of 128.)
ASTM E-1961 zone size is typically 1 mm to 3 mm.
Setup Automatic with file loading
Automated setup From file of weld profile or from predefined weld profile and appropriate parameters
Display

1. Conventional twin-gate strip chart display or
2. Increased number of zones for improved defect sizing or
3.Multiple B-scans for improved defect characterization or
4.Customized combination of displays Coupling and circumferential position channels included TOFD recommended

Calibration and codes ASTM E-1961, API 1104, or DNV2000-OS-F101 custom specifications
Additional modules For transverse defects, thick walls, dedicated TODF, and customized scans

Umbilical

Umbilical length Typically 25 m (80 ft)
Manufacture Armored cable 5 cm (2 in.) in diameter
Contents 128 ultrasonic cables, one motor drive cable, one encoder cable, and waterline for coupling

Phased Arrays

Instrumentation Standard Tomoscan FOCUS 32:128 system
(32 simultaneous pulsers, 128 channels)
Bandwidth 1 MHz to 20 MHz
Maximum pulsing rate 20 kHz PRF
Pulser delay Adjustable from 0 µs to 25 µs in 2-ns increments
Pulse output Amplitude from 50 V to 200 V, width from 20 ns to 500 ns
Receiver delay Adjustable from 0 µs to 25 µs in 2-ns increments
Receiver DAC Up to 30 dB/µs on each element slope before summing
Input filters Four user-selectable ranges:
None
500 kHz to 5 MHz
2 MHz to 10 MHz
5 MHz to 15 MHz
Input impedance 50 W
Inspection mode

Pulse-echo, transmit-receive (programmable)

Dynamic range 56 dB/channel
Computer interface Both RS-232 and Ethernet™ standard
Focal law storage Up to 1024 different laws
Power requirement 85 V to 265 V, 47 Hz to 63 Hz
Operating temperature 0°C to 50°C

この用途に使用される製品

PipeWIZARD

PipeWIZARDは、フェイズドアレイ法と従来のUT技術を組み合わせたパイプライン溶接部の自動検査システム(AUT)です。陸上や海上を選ばず、極めて厳しい環境下でも溶接部を次々と検査作業できるように設計されています。

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어