Industrial Testing Instruments

Trasduttori a fascio ultrasonoro angolare: applicazioni ad alta penetrazione

Prodotti ad ultrasuoni

Advantages

  • Wave layers with acoustic adaptation to Rexolite®
  • Captive anchoring screws are provided with the probe.
  • A wide selection of wedges is available to suit any angle beam application.

Typical applications

A3, A4, and A5 probes
Deep penetration applications

  • Thick plates and welds
  • Forging
  • Noisy or granular material

Probe specifications and dimensions

Part number

Frequency
(MHz)

Number of elements

Pitch
(mm)

Active
aperture (mm)

Elevation (mm)

External dimensions
mm (in.)

L

W

H

3.5L16-A3

3.5

16

1.60

25.6

16.0

36 (1.41)

36 (1.41)

25 (0.98)

5L16-A3

5.0

16

1.20

19.2

12.0

36 (1.41)

36 (1.41)

25 (0.98)

1.5L16-A4

1.5

16

2.80

44.8

26.0

57 (2.25)

46 (1.80)

30 (1.19)

2.25L16-A4

2.25

16

2.00

32.0

20.0

57 (2.25)

46 (1.80)

30 (1.19)

2.25L32-A5

2.25

32

0.75

24.0

24.0

29 (1.15)

43 (1.67)

24 (0.96)

5L32-A5

5.0

32

0.60

19.2

20.0

29 (1.15)

43 (1.67)

24 (0.96)

These probes come standard with an OmniScan® connector and a 2.5 m (8.2 ft) cable or can be specially fitted with other connectors and cable lengths.

English | 日本語 | français | 中文 | Deutsch | italiano | čeština | magyar | Español | русский | Tiểng Việt | polski | português