The OmniScan PA performs manual and automated phased array inspections. It offers full-featured A-scan, B-scan, S-scan and C-scan displays, and advanced real-time data processing. Configurable in 16:128 elements, also 16:16M, 16:64M, 32:32, and 32:128
Phased Array Technology

Phased array technology enables the generation of an ultrasonic beam where parameters such as angle, focal distance, and focal point size are controlled through software. Furthermore, this beam can be multiplexed over a large array. These capabilities open a series of new possibilities. For instance, it is possible to quickly vary the angle of the beam to scan a part without moving the probe itself. Phased arrays also allow replacing multiple probes and mechanical components. Inspecting a part
with a variable-angle beam also maximizes detection regardless of the defect orientation, while optimizing signal-to-noise ratio.
Benefits of Phased Arrays
Phased array technology offers the following benefits:
Full-Featured A-Scans, B-Scans, and C-Scans


The OmniScan® PA builds upon the OmniScan UT feature set and offers full-featured A-scan, B-scan, and C-scan displays.
Full-Featured Sectorial Scan


Advanced Real-Time Data Processing

Calibration Procedures and Parameters
All calibration procedures are guided by a step-by-step menu using Next and Back navigation.
Wizards for Groups and Focal Laws
Multiple-Group Option
It is now possible to manage more than one probe with two different configurations: different skews, different scanning types, different inspection areas, and other parameters.
Possible Configurations for Multiple-Group Inspection
A Use one single phased array probe of 64 or more elements and create 2 different groups:

B Use one single phased array probe of 64 or 128 elements and create 2 different groups:

C Use one phased array probe of 64 or 128 elements and create 3 different groups:

D Use two phased array probes of 16 or 64 elements and create 2 different groups:

* Models 16:16, 16:16M, 16:64M, 32:32, and 32:128 also available
| General | |
|
Overall dimensions
(W x H x D) |
244 mm x 182 mm x 57 mm
(9.6 in. x 7.1 in. x 2.1 in.) |
| Weight | 1.2 kg (2.6 lb) |
| Connectors |
1 OmniScan connector for phased-array probes
2 BNC connectors (1 pulser/receiver, 1 receiver for conventional UT) (BNC not available on models 32:32 and 32:128) |
| Number of focal laws | 256 |
| Probe recognition | Automatic probe recognition and setup |
| Pulser/Receiver | |
| Aperture | 16 elements* |
| Number of elements | 128 elements |
| Pulser | |
| Voltage | 80 V per element |
| Pulse width | Adjustable from 30 ns to 500 ns, resolution of 2.5 ns |
| Fall time | Less than 10 ns |
| Pulse shape | Negative square wave |
| Output impedance | Less than 25 Ω |
| Receiver | |
| Gain | 0 dB to 74 dB, maximum input signal 1.32 Vp-p |
| Input impedance | 75 Ω |
| System bandwidth | 0.75 MHz to 18 MHz (-3 dB) |
| Beamforming | |
| Scan type | Azimuthal and linear |
| Scan quantity | Up to 8 |
| Active elements | 16* |
| Elements | 128 |
| Delay range transmission | 0 µs to 10 µs in 2.5-ns increments |
| Delay range reception | 0 µs to 10 µs in 2.5-ns increments |
| Data acquisition | |
| Digitizing frequency | 100 MHz (10 bits) |
| Maximum pulsing rate | Up to 10 kHz (C-scan) |
| Acquisition depth | 29 meters in steel (L-wave), 10 ms with compression. 0.24 meter in steel (L-wave), 81.9 µs without compression |
| Data processing | |
| Number of data points | Up to 8000 |
| Real-time averaging | 2, 4, 8, 16 |
| Rectifier | RF, full wave, halfwave +, halfwave - |
| Filtering | Low-pass (adjusted to probe frequency), digital filtering (bandwidth, frequency range) |
| Video filtering | Smoothing (adjusted to probe frequency range) |
| Data storage | |
| A-scan recording (TOFD) | 6000 A-scans per second (512-point, 8-bit A-scan) |
| C-scan type data recording | I, A, B, up to 10 kHz (amplitude or TOF) |
| Maximum file size |
Limited to available internal flash memory:
180 MB (or 300 MB optional) |
| Data visualization | |
| A-scan refresh rate | Real-time: 60 Hz |
| Volume-corrected S-scan | Up to 40 Hz |
| Data synchronization | |
| On internal clock | 1 Hz to 10 kHz |
| On encoder | On 1 or 2 axes |
| Programmable time-corrected gain (TCG) | |
| Number of points | 16 (1 TCG curve per channel for focal laws) |
| Alarms | |
| Number of alarms | 3 |
| Conditions | Any logical combination of gates |
| Analog outputs | 2 |
This webinar reviewed the benefits of the new TomoView 2.9 software.
Request a quote for a custom phased array probe and/or wedge.
Copyright 2011 OLYMPUS CORPORATION, All rights reserved. Condizioni d'uso | Informativa sulla privacy