Inspection & Measurement Systems

Advanced NDT megoldások

PV-100

Pulse-Echo and TOFD Inspection Solution

The PV-100 is an advanced, automated weld inspection solution (AUT). Combines acquisition unit (OmniScan), scanner, encoder, and software. Designed to meet the productivity requirements of construction welding in petrochemical and power-generation industries. UT, TOFD, creeping wave.

The PV-100 solution is based on the proven OmniScan® UT flaw detector. This advanced UT instrument uses two inspection techniques simultaneously. The combination of time-of-flight diffraction (TOFD) and the pulse-echo or creeping wave technique allows a full volumetric inspection in a single pass.

Inspection results are available instantaneously providing immediate code based acceptance or rejection. This solution was specifically designed to meet the productivity requirements of construction welding in petrochemical and power-generation industries.

PV-100 attributes

  • Quickly detect weld defects
  • Accurately size defects
  • Easily characterize weld defects
  • Easily create customized reports
  • On site inspection without production disruption
  • Full data collection for auditing and code compliance

PV-100 Applications

  • Wind tower construction
  • Pressure vessel and piping construction
  • Structural construction welding
  • Structural welded components
  • Production control
  • In-service inspection of weld

PV-100 Specifications

Part thickness:8 mm up to 300 mm
Part diameter:100 mm up to flat
Part material:carbon steel

Available Scanners for PV-100 Solution

WeldROVER
HSMT-X03
HSMT-Flex

PV100

Pulse-echo channel, 60º shear wave for weld cap coverage.

PV100

Pulse-echo channel, 70º shear wave for weld root coverage.

PV100

TOFD channel for weld volume coverage.

PV100

Combining pulse-echo and TOFD channels offers complete coverage of the weld.

PV-100 Options

Umbilical cables

Two different umbilical cables are available:

  • The closed-type umbilical offers the most rugged protection. It covers the cable with a resistant, waterproof, and dust proof conduit.
  • The divisible type is composed of two split shells that protect the cables. Although not as rugged as the closed-type umbilical, it offers other advantages: the cables inside the umbilical can be changed at any time.

CFU03 - Electric Couplant-Feed Unit
The CFU03 is a portable electrical pump unit used to supply couplant to wedges during ultrasonic inspections.

WTR-SPRAYER-8L - Manual Couplant-Feed Unit
The manual feed unit offers a cheap and efficient way to supply couplant to wedges during automated inspections.

TRPP-5810 - Remote Pulser/Preamplifier for TOFD Inspection
The TRPP-5810™ unit is a high-performance remote pulser/preamplifier dedicated to TOFD inspections and compatible with Olympus industrial scanners.

Panametrics 5682 - Preamplifier for TOFD Inspection
The Panametrics 5682 ultrasonic preamplifier provides low-noise amplification of ultrasonic signals (for one probe) ranging from 500 kHz to 25 MHz.

Standard Inclusions

Contents of the PV-100 kit are configured depending on the thickness of the parts to inspect.

Typically a PV-100 kit consists of the following:

  • OmniScan® UT acquisition unit
  • UT probes and wedges
  • Industrial scanner
  • Encoder
  • Umbilical cable
  • Preamplifier
  • Irrigation system
Loading...

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어