Industrial Testing Instruments

Általános Célú Szögvizsgáló

Ultrahang

Angle beam probes are used with a wedge to transmit a refracted shear or longitudinal wave into a test piece. Designed for a wide range of applications, they can be used to vary the refracted beam angle or the skew of the beam, depending on the probe orientation.

Advantages

  • Probes are designed to have a low-profile probe/wedge combination for easier access in restricted areas.
  • Wave layers with acoustic adaptation to Rexolite®
  • Captive anchoring screws are provided with the probe.
  • A wide selection of wedges is available to suit any angle beam application.

Typical applications

A10, A11, and A12 probes

  • Manual or automated inspection of 6.35 mm to 38 mm (0.25 in. to 1.5 in.) thick welds
  • Detection of flaws and sizing
  • Inspections of castings, forgings, pipes, tubes, and machined and structural components for cracks and welding defects

Probe specifications and dimensions

Part number

Frequency
(MHz)

Number of elements

Pitch
(mm)

Active aperture (mm)

Elevation
(mm)

External dimensions
mm (in.)

L

W

H

5L16-A1

5.0

16

0.60

9.6

10.0

17 (0.67)

29 (1.16)

25 (0.98)

10L32-A1

10.0

32

0.31

9.9

7.0

17 (0.67)

29 (1.16)

25 (0.98)

5L64-A2

5.0

64

0.60

38.4

10.0

53 (2.09)

29 (1.16)

35 (1.38)

10L64-A2

10.0

64

0.60

38.4

7.0

53 (2.09)

29 (1.16)

35 (1.38)

5L16-A105.0160.609.610.016 (0.62)23 (0.89)20 (0.79)
10L32-A1010.0320.319.97.016 (0.62)23 (0.89)20 (0.79)
5L32-A115.0320.6019.210.016 (0.62)23 (0.89)20 (0.79)
5L64-A125.0640.6038.410.016 (0.62)23 (0.89)20 (0.79)
5L60-A145.0601.060.010.016 (0.62)23 (0.89)20 (0.79)
7.5L60-A147.5601.060.010.016 (0.62)23 (0.89)20 (0.79)

These probes come standard with an OmniScan® connector and a 2.5 m (8.2 ft) cable or can be specially fitted with other connectors and cable lengths.