Industrial Testing Instruments

Nagy Frekvenciás Vizsgálófejek

Ultrahang

Contact transducers are available in frequencies up to 225 MHz. Performance is dependent on pulser/receiver and application. All transducers are manufactured on a special basis to customer specifications. Contact us to discuss applications.

High Frequency Transducers

High frequency transducers are single element contact or immersion transducers designed to produce frequencies of 20 MHz and greater.

Advantages:

  • Heavily damped broadband design provides excellent time resolution
  • Short wavelengths for superior flaw resolution capabilities
  • Focusing allows for very small beam diameters
  • Frequencies range from 20 MHz to 225 Mhz

High Frequency Contact

  • Permanent fused silica delay line allows for flaw evaluation, material analysis or thickness measurements using a direct contact testing method
  • Three different delay line configurations (BA, BB, BC) allow for various combinations of delay line echoes
  • Standard connector style is Right Angle Microdot® (RM)

Freq

Nominal
Element Size

Delay

Transducer
Part Numbers

MHz

inches

mm

µsec

20

0.25

6

4.25

V212-BA-RM

0.25

6

4.25

V212-BB-RM

0.25

6

2.5

V212-BC-RM

30

0.25

6

4.25

V213-BA-RM

0.25

6

4.25

V213-BB-RM

0.25

6

2.5

V213-BC-RM

50

0.25

6

4.25

V214-BA-RM

0.25

6

4.25

V214-BB-RM

0.25

6

2.5

V214-BC-RM

0.125

3

4.25

V215-BA-RM

0.125

3

4.25

V215-BB-RM

0.125

3

2.5

V215-BC-RM

75

0.25

6

2.5

V2022 (BC)

0.125

3

2.5

V2025 (BC)

100

0.125

3

4.25

V2054 (BA)

0.125

3

2.5

V2012 (BC)

125

0.125

3

2.5

V2062

Please contact us for transducers in higher frequencies.


Transducer Dimensions
(in inches)

Delay Style

(A)

(B)

(C)

BA

0.72

0.81

1.00

BB

0.34

0.44

0.81

BC

0.34

0.44

0.63

High Frequency Standard Immersion Case

  • Permanent fused silica delay line
  • Focused units use an optical quality ground lens
  • F202 adaptor allows fixturing with a passive UHF connector and an active Microdot® style connector (see page 38)
  • Combines high frequency with a small case design

Freq

Nominal
Element Size

Delay

Focal
Length

Transducer
Part Numbers

MHz

inches

mm

µsec

inches

mm

20

0.25

6

4.25

flat

V354-SU

0.25

6

2.5

0.75

19

V372-SU

0.25

6

4.25

1.25

32

V373-SU

0.25

6

4.25

2.00

51

V374-SU

30

0.25

6

4.25

flat

V356-SU

0.25

6

2.25

0.75

19

V375-SU

0.25

6

4.25

1.25

32

V376-SU

0.25

6

4.25

2.00

51

V377-SU

50

0.25

6

4.25

flat

V358-SU

High Frequency SU/RM Immersion Case

  • Permanent fused silica delay with an optical quality ground lens provides a high degree of precision in beam alignment and focusing
  • Stainless steel case has a passive Straight UHF (SU) connector and an active Right Angle Microdot (RM) connector
  • Large cases allow for larger delay lines and decrease in delay reverberations and noise

Freq

Nominal
Element Size

Delay

Focal
Length

Transducer
Part Numbers

MHz

inches

mm

µsec

inches

mm

50

0.25

6

19.5

0.50

13

V390-SU/RM

0.25

6

19.5

0.75

19

V3192

0.25

6

19.5

1.00

25

V3193

0.25

6

19.5

1.75

45

V3409

0.25

6

19.5

2.00

51

V3337

0.25

6

9.4

0.20

5

V3330*

0.125

3

19.5

0.50

13

V3332

75

0.25

6

19.5

0.50

13

V3320

0.25

6

19.5

0.75

19

V3349

90

0.25

6

19.5

0.50

13

V3512

100

0.25

6

19.5

0.50

13

V3194

0.25

6

19.5

1.00

25

V3394

0.25

6

9.4

0.20

5

V3534*

0.125

3

10

0.25

6

V3346

*Transducers create surface waves in steel, titanium and other materials with similar velocities. Please contact us for higher frequency. Lightweight High Frequency transducers are an alternative to the SU/RM case style transducers. They offer a smaller case width and lighter weight without sacrificing performance.

English | 日本語 | français | 中文 | Deutsch | italiano | čeština | magyar | Español | русский | Tiểng Việt | polski | português