Industrial Testing Instruments

Szögvizsgáló-fejek

Ultrahang

Miniature Angle Beam Transducers and Wedges are used primarily for testing of weld integrity. Their design allows them to be easily scanned back and forth and provides a short approach distance.

Angle beam transducers are single element transducers used with a wedge to introduce a refracted shear wave or longitudinal wave into a test piece.

Advantages:

  • Three-material design of our Accupath wedges improves signal-to-noise characteristics while providing excellent wear resistance
  • High temperature wedges available for in-service inspection of hot materials
  • Wedges can be customized to create nonstandard refracted angles
  • Available in interchangeable or integral designs
  • Contouring available
  • Wedges and integral designs are available with standard refracted angles in aluminum

Applications:

  • Flaw detection and sizing
  • For time-of-flight diffraction transducers see page 25
  • Inspection of pipes, tubes, forgings, castings, as well as machined and structural components for weld defects or cracks


Miniature Screw-In Transducers

  • Screw-in design 303 stainless steel case
  • Transducers are color coded by frequency
  • Compatible with Short Approach, Accupath, High Temperature and Surface Wave Wedges

Nominal
Element Size

Freq.

Transducer Part Numbers

inches

mm

MHz

ACCUSCAN-S

CENTRASCAN

VIDEOSCAN

0.50

13

1.0

A539S-SM

C548-SM

V539-SM

2.25

A540S-SM

C540-SM

V540-SM

3.5

A545S-SM

C545-SM

V545-SM

5.0

A541S-SM

C541-SM

V541-SM

10

A547S-SM

-

V547-SM

0.375

10

1.0

A548S-SM

-

1.5

A548S-SM

-

-

2.25

A549S-SM

C549-SM

V549-SM

3.5

A550S-SM

C550-SM

V550-SM

5.0

A551S-SM

C551-SM

V551-SM

10

A552S-SM

-

V552-SM

0.25

6

2.25

A542S-SM

C542-SM

V542-SM

3.5

A546S-SM

C546-SM

V546-SM

5.0

A543S-SM

C543-SM

V543-SM

10

A544S-SM

C544-SM

V544-SM

Trasnducer Dimensions
(in inches)

Nominal Element Size

(A)

(B)

(C)

Thread Pitch

0.50

0.71

0.685

0.257

11/16 - 24

0.375

0.58

0.65

0.257

9/16 - 24

0.25

0.44

0.55

0.22

3/8 - 32

Accupath Wedges

  • Small wedge footprint
  • Pointed toe design allows transducer rotation even when the nose is touching a weld crown
  • Special wedge design for use with 10 MHz transducer

Miniature Screw-In Wedges for 1-5 MHz

Nominal
Element Size

Wedge Part Numbers

in

mm

Short Approach

Accupath*

High Temp*
500°F (260°C)

Very High Temp*
900°F
(480°C)

Surface Wave 90°

0.50

13

ABSA-5T-X°

ABWM-5T-X°

ABWHT-5T-X°

ABWVHT-5T-X°

ABWML-5T-90°

0.375

10

ABSA-7T-X°

ABWM-7T-X°

ABWHT-7T-X°

ABWVHT-7T-X°

ABWML-7T-90°

0.25

6

ABSA-4T-X°

ABWM-4T-X°

ABWHT-4T-X°

ABWVHT-4T-X°

ABWML-4T-90°

Miniature Screw-In Wedges for 10 MHz Transducers

Nominal
Element Size

Wedge Part Numbers

inches

mm

Short Approach

Accupath*

Surface Wave 90°

0.50

13

ABSA-5T-X°

ABWM-5ST-X°

ABWML-5ST-90°

0.375

10

ABSA-7T-X°

ABWM-7ST-X°

ABWML-7ST-90°

0.25

6

ABSA-4T-X°

ABWM-4ST-X°

ABWML-4ST-90°

Short Approach Wedges are available in standard refracted shear wave angles of 45°, 60°, and 70° in steel at 5.0 MHz.

*Accupath Wedges are available in standard refracted shear wave angles of 30°, 45°, 60°, and 70° in steel at 10 MHz.

Accupath and Surface Wave Wedge Dimensions* (Miniature Screw-in)

Fits Nominal Element Size (in inches)

0.5

0.375

0.25

(A)

(B)

(C)

(D)

(A)

(B)

(C)

(D)

(A)

(B)

(C)

(D)

30°

0.72

1.22

0.77

0.54

0.62

1.03

1.03

0.42

0.49

0.66

0.45

0.23

45°

0.70

1.03

0.73

0.38

0.60

0.85

0.61

0.32

0.43

0.61

0.43

0.235

60°

0.74

1.19

0.73

0.45

0.67

1.00

0.61

0.367

0.48

0.71

0.43

0.268

70°

0.79

1.34

0.73

0.50

0.69

1.12

0.61

0.406

0.50

0.81

0.43

0.305

90°

1.25

1.84

0.77

-

1.00

1.48

1.48

-

0.83

1.13

0.45

-

Short Approach Wedges

  • Smallest footprint
  • Short approach distance allows for inspection closest to the weld crown

Short Approach Wedge Dimensions (Miniature Screw-in)

Fits Nominal Element Size (in inches)

0.5

0.375

0.25

(A)

(B)

(C)

(D)

(A)

(B)

(C)

(D)

(A)

(B)

(C)

(D)

45°

0.70

1.03

0.73

0.38

0.60

0.85

0.61

0.32

0.43

0.61

0.43

0.235

60°

0.74

1.19

0.73

0.45

0.67

1.00

0.61

0.367

0.48

0.71

0.43

0.268

70°

0.79

1.34

0.73

0.50

0.69

1.12

0.61

0.406

0.50

0.81

0.43

0.305

English | 日本語 | français | 中文 | Deutsch | italiano | čeština | magyar | Español | русский | Tiểng Việt | polski | português