december 08, 2009 Olympus Provides a Comprehensive Weld Inspection Solution for Pipes with a Diameter as Small as 0.84 in. (21.3 mm)
Olympus, a world leader in nondestructive testing technologies and pioneer in industrial phased array ultrasound, is pleased to introduce a comprehensive inspection solution for circumferential welds in pipes with a diameter as small as 0.84 in. (21.3 mm) OD. A key component of the solution is the COBRA, a new manual scanner specifically designed to inspect welds in small diameter pipes. The COBRA is used with the OmniScan® MX Phased Array flaw detector with the 16:128 module and the
OmniScan MXU software, to provide an economical and portable weld inspection solution.
|