The use of ultrasonic thickness gauges can provide many advantages when a mill operator has to verify wall thickness of an extruded pipe or tube. In the mill, nondestructive wall thickness measurements of the pipe can be made to detect out-of-tolerance conditions. Concentricity of an extruded pipe can be monitored on a continuous and automatic basis with no need to cut the pipe or to shut down the manufacturing process. Similarly, when a machinist needs to accurately measure the thin wall of a tube, ultrasonics permits nondestructive thickness measurements along the total length.

Equipment: For manual thickness measurements, the Model 35DLand Model 38DL PLUS gages provide instant digital readings of most metal pipes and tubes to a calibrated accuracy of ±0.001 inch (±0.025 mm). This model used with an M112 contact transducer is capable of measuring most metal walls ranging from 0.020 to 1 inch (0.50 to 25.0mm). The Model 35 can also be used in situations where data logging is not required.

If the diameter of a tube is less than 0.125 inch (3mm), we recommend the Model 35DL or 38DL PLUS with an immersion transducer. The Model RBS-1 Bubbler System is a helpful tool in making ultrasonic thickness measurements that utilize immersion transducers. The 35DL and 38DL PLUS can be used with delay line transducers to make thickness measurements to a calibrated accuracy of ±0.0002 inch or ±0.005 mm.

Wall thickness measurements on metal pipes or tubes that are badly corroded on either the inside or the outside surface should, as a rule, be made with the Panametrics-NDT Model 38DL PLUS, or the MG2 series.

Products used for this application

35DL

The pocket-sized 35DL is a handheld ultrasonic thickness gage for precision measurements on metal, plastic, rubber, glass, and composites using single element transducers. Same features as Model 35 but has internal datalogger.

38DL PLUS

The 38DL PLUS is an advanced ultrasonic thickness gage. Uses dual element transducer for internally corroded applications, features include THRU-COAT and Echo-to-Echo. Uses single element transducers for very precise thickness measurements of thin, very thick, or multilayer materials.

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어