Inspection & Measurement Systems

Felhasználás

Application Notes

Titánium Öntvények Vizsgálata Fázisvezérelt Ultrahanggal

General description of the application

Some aircrafts structural part such as engine mount and frame are now built with titanium casting. This material is very difficult to inspect because of its large grain structure. The usual inspection methods are X-ray and ultrasounds, however they present some limitations.
The use of ultrasound phased arrays brought a break­through in the inspection of casting by providing a much better detectability than the conventional methods.

Typical inspection requirement
• Finding and characterizing inclusions
• Covering casting part volume completely
• Flexible enough to fit various shapes
• Portable to perform inspections in-service or in-production

Defects detected
• Ceramic shell as small as 0.031 in. at a 1-in depth
• Tungsten carbide as small as 0.031 in at a 1-in. depth

Description of the solution
• Phased array probe steering the beam from -30°to 30°LW
• Merged top and side views
• 10 and 5 MHz linear phased array probe

Description of the inspection system
• Focus 32:32 or more
• Dynamic Depth Focusing option
• Linear phased array probe
• Manual or automated X-Y scanner

Parts to inspect
• Engine mount
• Frame
• Thickness: 1 to 6 inches

Method of inspection
The phased array probe steers the beam continuously between -30°to 30°LW with an angular resolution of 1 degree. It allows the detection of orientated inclusions. Dynamic Depth Focusing is applied to keep the beam focused over the depth range. The probe scans a X-Y surface and data is merged together to create a top-side view of the casting part. Analysis is performed.

Advantages
• Better detectability than X-ray (The smallest defect detected by X-ray is 0.065 in; by UT phased arrays, it is 0.031 in.)
• Versatility
• Fast and easy to use


Detection of ceramic schells. Merged top- and side-views display.


GLIDER scanner


TomoScan FOCUS LT

Products used for this application

GLIDER Scanner

The GLIDER scanner is a 2-axis (X-Y) encoding scanner for the manual inspection of slightly curved or flat composite surfaces. The scanner, held by suction cups is well suited for raster scanning. Technologies: ECA, EC, UT, PA.

TomoScan Focus LT

The TomoScan FOCUS LT is designed for most demanding automated and industrial inspection systems for both conventional UT and phased array with multiple probe configuration. It is controlled by the versatile TomoView software.

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어