Dupla Varrat AUT VIZSGÁLATA PipeWIZARD™-al

Meets or exceeds API 1104, DNV 2000, OS101, and ASTM E-1961 AUT codes

  • Proven and qualified AUT system for double and quadruple jointing at mill, as well as onshore and offshore pipeline construction
  • Safe system: no radiation hazard
  • Efficient system: no disruption of normal operation
  • Money-saving system: better process control of welding, giving lower reject rates
  • Better weld quality with unique system performance
  • High defect detection capability
  • Extra beams for key areas, such as root passes
  • Any weld profile: CRC-Evans, J-bevel, modified J-bevel, V,double V .
  • Better productivity
  • Wide range of pipe diameters and wall thicknesses
  • Fast scanning speed: 100 mm/s
  • Cycle time of approximately two minutes for 36-inch pipe welds
  • Rapid data interpretation (virtually in real-time)




PipeWIZARD phased-array automated ultrasonic inspection system (AUT).


Lack of fusion detection confirmed by macrophotography.


Ultrasonic zone discrimination is a key feature of AUT with PipeWIZARD.

System Description
  • Tomoscan FOCUS™ 32:128 phased-array unit
  • Motor drive unit
  • Industrial PC
  • Downsized probe pan containing two linear arrays
  • Mechanized drive clamping onto welding band
  • 25 m umbilical cable connecting probes, encoder, power, and couplant lines to instrumentation
  • Instrumentation console including PC, pulsers, and motor drive
  • Couplant containers, pump, and reclamation unit


Probe Pan Description
  • Probe pan contains two linear arrays.
  • Extra modules are available for transverse or dedicated TOFD inspections.
  • Couplant is pumped water or water-methanol in cold climates.
  • Encoder running on welding band gives circumferential position.

    Software Description
  • Custom PipeWIZARD™ software running on Microsoft® Windows NT® for data acquisition, analysis, and reporting
  • Automatic marking of indications exceeding rejection threshold to assist the operator
  • Inspection reports and list of defects adapted to client requirements
  • Automatic saving to two separate media in real time
  • Automated inspection sequence

PipeWIZARD

Pipe diameter 50 mm to 1424 mm (2 in. to 56 in.)
Pipe wall thickness 6 mm to 36 mm (0.25 in. to 1.5 in.) or more depending on wall thickness and addtional transducers. (Additional transducers may be required.)
Array Two linear 7.5-MHz, 60-element, 75 mm long
Scan speed 100 mm/s (4 in./s)
Scanner size 250 mm (L) x 120 mm (W) x 75 mm (H)
Scanner weight 2 kg (4 lb)
Additional probe pan slots Extra slots for eight conventional transducers for transverse defects or additional scans
Weld profile All common welds: CRC-Evans, J-bevel, manual, V, double V, X, etc. (any profile in principle)

Ultrasonics

Method Multichannel zone discrimination or custom scans as specified
Zone size <1 mm possible using increased number of zones.
(Maximum number of zones is 32 per view, and four views are available for a total of 128.)
ASTM E-1961 zone size is typically 1 mm to 3 mm.
Setup Automatic with file loading
Automated setup From file of weld profile or from predefined weld profile and appropriate parameters
Display

1. Conventional twin-gate strip chart display or
2. Increased number of zones for improved defect sizing or
3.Multiple B-scans for improved defect characterization or
4.Customized combination of displays Coupling and circumferential position channels included TOFD recommended

Calibration and codes ASTM E-1961, API 1104, or DNV2000-OS-F101 custom specifications
Additional modules For transverse defects, thick walls, dedicated TODF, and customized scans

Umbilical

Umbilical length Typically 25 m (80 ft)
Manufacture Armored cable 5 cm (2 in.) in diameter
Contents 128 ultrasonic cables, one motor drive cable, one encoder cable, and waterline for coupling

Phased Arrays

Instrumentation Standard Tomoscan FOCUS 32:128 system
(32 simultaneous pulsers, 128 channels)
Bandwidth 1 MHz to 20 MHz
Maximum pulsing rate 20 kHz PRF
Pulser delay Adjustable from 0 µs to 25 µs in 2-ns increments
Pulse output Amplitude from 50 V to 200 V, width from 20 ns to 500 ns
Receiver delay Adjustable from 0 µs to 25 µs in 2-ns increments
Receiver DAC Up to 30 dB/µs on each element slope before summing
Input filters Four user-selectable ranges:
None
500 kHz to 5 MHz
2 MHz to 10 MHz
5 MHz to 15 MHz
Input impedance 50 W
Inspection mode

Pulse-echo, transmit-receive (programmable)

Dynamic range 56 dB/channel
Computer interface Both RS-232 and Ethernet™ standard
Focal law storage Up to 1024 different laws
Power requirement 85 V to 265 V, 47 Hz to 63 Hz
Operating temperature 0°C to 50°C

Products used for this application

PipeWIZARD

The PipeWIZARD is an automated girth weld inspection system using phased array and conventional UT techniques (AUT). Specially designed for in-site weld-to-weld inspection in extreme environments, on-shore and off-shore.