Applications

Notes d’application

Determination of Calcium, Zinc, Sulfur, and Phosphorus in Lubricating Oils

Critical to protect precision equipment operating under extreme temperatures and heavy loads, top quality lubricants depend on specially formulated blends of organo-metallic additives. These additives extend lubricant life, protect metal surfaces and increase the range in which a lubricant can be used. Additive elements such as calcium and zinc contribute to key lubrication characteristics; sulfur and phosphorus key to extreme pressure lubricants. A sound maintenance program that routinely measures metals in the lubricating oils not only reduces the expense of routinely dismantling the components for visual inspection, but can indicate and identify the worn component before that component fails.

The X-5000 will provide a quick determination to ensure your lubricants and fuels are in the best possible condition prior to use. The X-5000 allows for instant analysis, providing vital information at that precise moment and not weeks later. Wear metals such as Cu, Fe, Ni and V in engine oils, and the verification of additive elements for depletion - P, Ca, Zn - key lubrication characteristics. Routine testing identifies those small problems before they become costly failures.

The X-5000 sets the benchmark for Performance, Power and Portability. No sample preparation, just collect it and analyze - right on the spot.

lube

X-5000 closed chamber

Key Feature and Benefits

  • Portable and lightweight
  • Fits on any lab bench, at the work site, inspection line, production area
  • Sample positioning tray accommodates all sample cups/bottles
  • No sample preparation required
  • No daily calibrations
  • Starts up immediately, results are displayed in seconds
  • Closed beam operation for user safety
  • Data is stored automatically in tamper-proof format

The unique sample tray ensures proper placement of the sample every time for accurate analysis. The sample tray accommodates both bottles and cups of any size.

X-5000 testing petroleum

The X-5000 is engineered to be used anywhere - in the field, at the production line, in an inspection area. It ensures operator safety as a fully interlocked, closed beam system. The closed beam, integrated design unique to the X-5000 is a critical safety advancement as portable XRF analyzers continue to increase in x-ray power and be applied to ever more demanding, in-the-field analytical challenges.

The X-5000 is your answer for the best analytical performance without compromising field portability or operator safety.

Element Detection Limits

Element LOD (ppm)
(180 s)
Phosphorus 30
Sulfur 12
Chlorine 15
Molybdenum 1
Calcium 5
Vanadium 1
Manganese 1
Iron 1
Cobalt 1
Nickel 1
Copper 1
Zinc 1
Mercury 1
Arsenic 1
Lead 1
Selenium 1

The analytical performance, closed beam safety and ease of use of traditional bench top XRF units are all captured in the X-5000. And it delivers true field portability, being packaged into an easy to carry, 22 lb. battery operated XRF with integrated PC and industrialized large touch screen.

Specifications

Concentration Range ppm to % levels
Analyzer Weight 10 kg (22 lbs)
Measurement Time 180 s
Operating Environment -10 to 50 °C
Power Requirements AC or Battery
Tube Voltage 10 - 50 kV
Tube Current 200 µA
User Interface Built in Touchscreen
Instrument Dimensions 38 x 33 28 cm
(15 x 13 x11 in.)
Sample Chamber 29 x 11 x 15 cm
(11 x 6 x 5 in.)

Products used for this application

Système XRF mobile X-5000

Le système XRF portable X-5000 offre la puissance et la performance d'analyse EDXRF d'un appareil de laboratoire dans un boîtier portable : à tube, boîtier fermé, ordinateur embarqué, grand écran et clavier virtuel. Pesant 12,7 kg sans batterie, il est idéal pour l'analyse des liquides, des solides ou des poudres dans les laboratoires mobiles ou sur les lignes d'inspection de matériel entrant ou sortant.

Inspection & Measurement Systems
English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어

Solutions avancées NDT

Appareils US de recherche de défauts

Systèmes intégrés d'inspection

Analyseurs XRF et XRD