Application: Testing the integrity of metallic braze joints in metal tubing and other parts.

Background: Brazing is a common process for joining sections of small diameter metal tubing and certain other small metal parts such as electrical contacts. It bonds two pieces of metal by means of a metallic filler that is melted and then flowed into the space between them by capillary attraction. The process is similar to soldering. The filler metal, which is commonly an alloy of copper, silver, tin and/or zinc with a relatively low melting point, must fill the space between the two parts being joined, wet the surfaces, and fuse them when it cools and solidifies. If the braze metal does not flow properly or does not fuse, the integrity of the joint will be affected. This problem can usually be identified with an ultrasonic flaw detector.

Equipment: Most braze joints can be tested with any Olympus ultrasonic flaw detector, including the EPOCH LTC, EPOCH 600, EPOCH XT, and EPOCH 1000. Given the typical geometry of braze joints, small diameter contact or delay line transducers are usually used. The transducer should be selected with respect to the geometry of the specific joint being tested, but for typical small diameter tubing the V208-RM (20 MHz) and V260 Sonopen (15 MHz) transducers are most commonly recommended.

Procedure: Braze joints are typically tested by means of a straight beam test that monitors the amplitude of the echo from the inside surface of the outer metal part. In the case of a good braze joint at the test point, the metal-to-metal bond will return a relatively small reflection, while an air gap will return a much larger one. These levels are established in each case by setting up on samples representing know brazed and un-brazed conditions.

The example below represents typical echoes from a braze joint between 9.5 mm (.0375 in.) and 12.5 mm (0.5 in.) copper tubing that was tested with a V208-RM transducer and an Epoch XT flaw detector. The first waveform shows a reference echo from an un-brazed area of the outer tube, which has been marked with a gate and set to nearly full screen height. The second waveform shows the response from a properly brazed point, in which the echo in the gated region drops to a very low level. By observing the amplitude of the echo within the gate, the operator can determine the joint condition at each test point by comparing the echo amplitude to these reference levels.

A partial braze within the area of the sound beam will be represented by a mid-level echo. Note: it is important to remember that very small discontinuities such as pinholes whose size is a small fraction of the beam diameter will not be detected through this procedure.

unbrazed joint screen

Typical echo response from unbrazed point.

brazed joint screen

Typical echo response from brazed point.

Products used for this application

Série EPOCH 1000

L’EPOCH 1000 est un appareil de recherche de défauts par ultrasons haute performance qui peut accueillir des fonctionnalités d’imagerie multiéléments. La modification de l’appareil se fait à un centre de service autorisé d’Olympus. Ses fonctionnalités clés sont la conformité EN12668-1, un jeu de 37 filtres numériques et une fréquence de récurrence de 6 kHz pour l'inspection à haute vitesse.

EPOCH 600NEW

L’EPOCH 600 est un appareil de recherche de défauts par ultrasons de niveau intermédiaire. D’un poids de seulement 1,68 kg, son boîtier horizontal est construit pour résister aux rigueurs des environnements très difficiles. Sa fonction EN12668-1 inclut l’émetteur carré réglable PerfectSquareTM de 400 V, le filtrage numérique qui améliorer le rapport signal sur bruit.

EPOCH LTC

L'EPOCH LTC est un appareil de recherche de défauts par ultrasons portable intermédiaire intégré dans un boîtier vertical de 0.96 kg. Il s'agit d'un appareil complet offrant la conformité EN12668-1, une grande variété de caractéristiques de série et des options spécialisées qui pourront répondre à vos besoins d'inspection.

EPOCH XT

L'EPOCH XT est un appareil de recherche de défauts par ultrasons portable de pointe intégrant de nombreuses fonctionnalités de mesure standard, y compris un émetteur carré réglable, des filtres numériques bande étroite et large bande sélectionnables, une étendue de gain de 0 dB à 110 dB, la fonction de mémoire de crête et de maintien de crête et une fréquence de récurrence réglable.

Inspection & Measurement Systems
English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어

Solutions avancées NDT

Appareils US de recherche de défauts

Systèmes intégrés d'inspection

Analyseurs XRF et XRD