| General Description of the Application There are innumerable welded tubes and pipes in the oil and gas industry. From manufacture through the entire service life of these welded parts, they must be inspected and monitored because of pressure and toxic contents. Magnetic particle inspections are frequently used, but this technique is limited to surface or breaking defects. X-ray technique is also used, but is time consuming and requires a safety zone around the inspection area. For these reasons, the use of ultrasonic inspections using the OmniScan™ Phased Array unit, manual scanner and 64-element probe provides major benefits: the most precise results, best images, fast inspections, and a nonhazardous inspection technique. Typical Inspection Requirements
Type of Defects
Description of the Solution
Advantages of the Solution
Equipment Required
Prior to any inspection conforming to the ASME code, a performance demonstration is required. A zero-degree scan is performed on the near-weld material and the heat-affected zone (HAZ) to make sure the ultrasonic beam from the phased-array probe will penetrate the welded area properly. This scan is also used to find any laminations. A first inspection is performed using a linear scan with an electronic scan using a 60-degree SW covering the complete volume of the weld. Then a second scan is made using a 70-degree SW. The same two angles are reused on the other side of the weld. A first data analysis is made on the OmniScan™ after each scan. If an indication is found, the file is imported into TomoView™ where the indications are sized and characterized.
|
El OmniScan PA permite realizar inspecciones phased array manuales y automatizadas. Ofrece todas las funcionalidades de las pantallas A-scan, B-scan, S-scan y C-scan, así como el tratamiento de datos en tiempo real de avanzada. Permite configuraciones con elementos 16:128 y la posibilidad de 16:16M, 16:64M, 32:32 y 32:128
El detector de defectos phased array OmniScan MX2 con interfaz de pantalla táctil permite aumentar la eficiencia de los ensayos. Incluye nuevas y potentes herramientas software que aseguran rendimientos superiores en aplicaciones manuales y automáticas avanzadas, con configuraciones, ciclos de ensayos y creación de informes más rápidos. Es compatible con todos los módulos phased array existentes.Copyright 2011 OLYMPUS CORPORATION, todos los derechos reservados. Condiciones de uso | Política de privacidad