Application

In the die casting process, molten metal flowing into the mold may harden before it is fused completely, producing shallow wrinkles on the die-cast surface. This phenomenon is known as ripple marks. The ripple marks are problematic because they distort the external appearance of the product and may cause damage or deformation when stress is applied.

The Olympus solution

Olympus' LEXT 3D laser scanning microscope makes it easy to accurately image a three-dimensional surface profile down to the micron level. Users can perform defect management using numerical surface roughness data, which is the best method for quality control. With the LEXT’s image stitching feature, users can create high-contrast images of the entire defect location. Moreover, because the microscope is contactless, the object’s surface will not be scratched.

Non-defective surface

laser_non-defective_surface_bf

laser_non-defective_surface_3D

Objective lens 20X, Zoom 1X; 6×3 stitching

Defective surface

laser_defective_surface_bf

laser_defective_surface_3D
 

Olympus IMS

Productos para la aplicación
NEW

El microscopio de escaneo láser LEXT™ OLS5100 combina precisión y rendimiento óptico a un nivel excepcional junto con herramientas inteligentes que facilitan su uso. Las tareas de medición precisa y submicrométrica con respecto a la forma y la rugosidad superficial son rápidas y eficientes, lo que simplificará su flujo de trabajo y proporcionará datos de alta calidad en los que puede confiar.

Lo sentimos, la página solicitada no se encuentra disponible en su país.
Let us know what you're looking for by filling out the form below.
Lo sentimos, la página solicitada no se encuentra disponible en su país.