Industrial Testing Instruments

Angle Beam - Small-Footprint and Near-Wall Probes

Ultrasound Products

Advantages of small-footprint probes

  • Access to confined areas (A00 probe has an 8 × 8 mm footprint)
  • Cable connector can come out from either the side or the top (A0 only).
  • Special-design small-footprint wedge
  • 10L16-A00 is used for aerospace scribe-mark applications.

Advantages of near-wall probes

  • Shortened dead zone at both ends (1.5 mm between center of first or last element and housing edge)
  • Well suited for composite channel inspections
  • Used for C-scan inspections of composites (delamination, disbonding, and porosity)

Probe specifications and dimensions

Part number

Frequency
(MHz)

Number of elements

Pitch
(mm)

Active
aperture (mm)

Elevation
(mm)

External dimensions
mm (in.)

L

W

H

Small-footprint probes

10L16-A00

10.0

16

0.31

5.0

5.0

8 (0.31)

8 (0.31)

23 (0.90)

5L10-A0-SIDE

5.0

10

0.60

6.0

6.0

13 (0.50)

10 (0.40)

23 (0.90)

5L10-A0-TOP

5.0

10

0.60

6.0

6.0

13 (0.50)

10 (0.40)

23 (0.90)

10L10-A0-SIDE

10.0

10

0.60

6.0

6.0

13 (0.50)

10 (0.40)

23 (0.90)

10L10-A0-TOP

10.0

10

0.60

6.0

6.0

13 (0.50)

10 (0.40)

23 (0.90)

Near-wall probes

3.5L64-NW1

3.5

64

1.0

64.0

7.0

66 (2.60)

19 (0.75)

25 (0.98)

5L64-NW1

5.0

64

1.0

64.0

7.0

66 (2.60)

19 (0.75)

25 (0.98)

3.5L24-NW2

3.5

24

1.0

24.0

7.0

22 (0.85)

19 (0.75)

30 (1.18)

5L24-NW2

5.0

24

1.0

24.0

7.0

22 (0.85)

19 (0.75)

30 (1.18)

3.5L128-NW3

3.5

128

1.0

128.0

7.0

130 (5.12)

21 (0.83)

35 (1.38)

5L18-NW3

5.0

128

1.0

128.0

7.0

130 (5.12)

21 (0.83)

35 (1.38)

These probes come standard with an OmniScan® connector and a 2.5 m (8.2 ft) cable or can be specially fitted with other connectors and cable lengths.