Batches of coiled steel often need to be inspected for compliance with thickness specifications. Conventional measurements are limited to the cut edges at the head of the coil. Ultrasonic thickness measurements, on the other hand, are made from one side only - the exposed side - making it possible to monitor the thickness over the entire width of the coil. Since the thickness can vary as much as 0.002 to 0.004 inch (0.05 to 0.10mm) from edges to center, steel processors find great advantages in using small ultrasonic gauges.

Equipment: Selection of instrumentation depends on the accuracy that is required. The best accuracy can be achieved with the Model 35DLorModel 38DL PLUSgages with a 20 MHz (M208) or 10 MHz (M202) delay line transducer. In general, the calibrated accuracy with the Model 35DL or Model 38DL PLUS combined with an M116 contact transducer is ±0.001 inch (±0.01mm). In the High Resolution Mode with an M208 or M202 delay line transducer this gage is capable of approaching a calibrated accuracy of ±0.0003 inch (±0.008mm) or better if thickness measurements are taken with delay line transducers under optimum circumstances.
Continuous on-line thickness gaging can also be applied to coiled steel, using immersion type transducers. Contact us for details.

Products used for this application

35 Series

General purpose, lightweight Panametrics gauges feature optional live Waveform and Adjust Mode. 35DL and 35DL-HP have alphanumeric data logger.

38DL PLUS

The versatile 38DL PLUS can be used with dual element transducers for the measurement of corroded pipes to the very precise thickness measurements of thin or multilayer materials with a single element transducer.

English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Español | русский | Tiểng Việt | polski | português | 한국어