The sub-miniature (HS-225) and ultra-miniature (HS-877) angle beam transducers are supplied in frequencies from 2.25 to 10.0 MHz with angles from 45° through 90°. Epoxy housings prevent the transducer from causing scratches to the test surface. These transducers are ideal for inspection of small diameter welded tubes and applications where the requirement is for a shear-wave transducer with a very small footprint. Depending on the type selected, either top or side mounted, Microdot connectors
are available. When ordering, please specify part number, frequency, angle, material to be inspected, and connector location.

 |
Transducer Housing Dimensions
Sub-Miniature: 0.375 in. L x 0.425 in. H x .0325 in. W
Ultra-Miniature: 0.375 in. L x 0.375 in. H x 0.250 in. W |
Size | Frequency (MHz) | Material | Connector | Angle
XX = Specify Angle |
0.120" x 0.250"
3 mm x 6 mm | 2.25 | Aluminum | Straight | HS-225-2-
XX-AL-SM |
2.25 | Aluminum | Right Angle | HS-225-2-XX-AL-RM |
2.25 | Steel | Straight | HS-225-2-XX-ST-SM |
2.25 | Steel | Right Angle | HS-225-2-XX-ST-RM |
5.0 | Aluminum | Straight | HS-225-5-XX-AL-SM |
5.0 | Aluminum | Right Angle | HS-225-5-XX-AL-RM |
5.0 | Steel | Straight | HS-225-5-XX-ST-SM |
5.0 | Steel | Right Angle | HS-225-5-XX-ST-RM |
10 | Aluminum | Straight | HS-225-10-XX-AL-SM |
10 | Aluminum | Right Angle | HS-225-10-XX-AL-RM |
10 | Steel | Straight | HS-225-10-XX-ST-SM |
10 | Steel | Right Angle | HS-225-10-XX-ST-RM |
0.187" x 0.187"
5 mm x 5 mm | 2.25 | Aluminum | Straight | HS-877-2-XX-AL-SM |
2.25 | Aluminum | Right Angle | HS-877-2-XX-AL-RM |
2.25 | Steel | Straight | HS-877-2-XX-ST-SM |
2.25 | Steel | Right Angle | HS-877-2-XX-ST-RM |
5.0 | Aluminum | Straight | HS-877-5-XX-AL-SM |
5.0 | Aluminum | Right Angle | HS-877-5-XX-AL-RM |
5.0 | Steel | Straight | HS-877-5-XX-ST-SM |
5.0 | Steel | Right Angle | HS-877-5-XX-ST-RM |
10 | Aluminum | Straight | HS-877-10-XX-AL-SM |
10 | Aluminum | Right Angle | HS-877-10-XX-AL-RM |
10 | Steel | Straight | HS-877-10-XX-ST-SM |
10 | Steel | Right Angle | HS-877-10-XX-ST-RM |
Specify material to be inspected. |