Portable XRF for Analysis of Dental Scrap

Introduction

Dental alloys are alloys specially developed for the dental industry. They often contain precious metals like Gold, Silver, Platinum and Palladium.

In the dental field, there are now far more than 1000 different alloys, with the precious metal alloys (high-gold, gold-reduced, palladium-based and silver-base alloys) in the majority.

These elements form the basic material for the dental alloys used in amalgams, crowns, bridges and other dental fittings. Once removed, they are a valuable precious metals resource. Together, with other precious metal scrap (x-ray fixers and films, castings and their materials, trap filters, wipes,sweeps, and grindings from bench work), these products are processed by precious metal refiners. Compositional analysis is a critical part in the valuing and quality control of these materials. Not only is a visual test unreliable, but the weigh difference between karats may be negligible.

gold teeth (bridge)

In addition, analyzing dental gold by using conventional gold-purchase acids is difficult; the acid method which works for jewelry might not necessarily work for dental alloys, as they contain non-traditional alloying elements.

The optimal analysis method for assaying dental alloys is X-Ray Fluoresence (XRF), a fast, precise, and nondestructive analytical technique.

Olympus Innov-X XRF Analyzers

Performance You Can Count On

In an economic environment where fast AND accurate results are more important than ever, the GoldXpert form Olympus Innov-X provides optimized precision and accuracy.

close-up of GoldXpert sample chamber

The GoldXpert is a crossover XRF analyzer, of offering benchtop analyzer performance and sensitivity with the convenience and mobility of a battery powered portable analyzer.

The GoldXpert has an integrated PC, and only weighs 10 kg (22lbs). Its internally lit chamber allows sample viewing during tests, and offers an articulating sample holder for even the most unusually shaped pieces.

GoldXpert with sample in chamber

The GoldXpert can be configured specifically for the measurement of precious metals in dental alloys. In addition to Au, Ag, Pt, and Pd the GoldXpert provides high level of performance of other elements like Ti, Cr, Mn, Fe, Ni, Cu, Zn, Ru, Rh, Zr, W, Ga, In, and others.

teeth

Typical performance on dental alloys

ASSAY GoldXpert Difference ASSAY GoldXpert Difference
Sample Au % Au % Au -/+ Pd % Pd % Pd +/-
1 41.95 41.84 0.19 5.18 4.91 0.05
2 32.69 32.41 0.17 7.19 7.24 0.05
3 36.54 36.32 0.15 6.93 6.73 0.04
4 50.65 50.51 0.18 6.68 6.22 0.05
5 38.42 38.41 0.14 12.52 12.31 0.05
6 29.82 29.76 0.13 16.83 16.51 0.06
7 23.63 23.43 0.12 17.91 17.91 0.07

GoldXpert Basic Specifications
Weight approximately 22 lb (10 kg)
Size 267 x 350 x 330 mm closed chamber
Analysis chamber size 125 x 210 x 180 mm with leaded glass viewing window and internal LED light
Source 4W Au / Ta target X-ray Tube
Detector Si-PIN (standard) /SDD (optional)
Calibration Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Ge, Zr, Nb, Mo, Ru, Rh, Pd, Ag, Cd, Sn, Sb, Hf, Ta, W, Re, Ir, Pt, Au, Pb, Bi, Ga, Se, In
(optional SDD instrument adds Os or other)
Processor 500 MHz Dual Core DSP, 530 MHz CPU
Power AC power or Rechargeable Li-Ion Battery
Standard battery life is < 3 hours operation
Display 32 bit color QVGA display (high brightness touch-screen) 57 x 73 mm
Memory Miscro SD 2GB memory (can store more than 150,00 data)
Communication USB, Bluetooth
Sample Viewing 3 mm small spot collimation for fine focusing (10 mm standard spot)

Products used for this application

GoldXpert Mobile XRF AnalyzerNEW

The GoldXpert is a stylish countertop analyzer fit for the consumer showroom environment. Designed to be compact and lightweight, weighing only 22 lbs (10kg), the GoldXpert can be transported easily to wherever testing is needed. The GoldXpert gives accurate chemistry and karat results within seconds.

Inspection & Measurement Systems
English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어

Advanced NDT Solutions

Flaw Detectors

Integrated Inspection Systems