Inspection & Measurement Systems

Ultraschallprüfgeräte

Magnetic Flux Leakage Probes

Sonde_Tube_CF_TFB179_02.psd

Sonde_Tube_CF_TFB179_01.psd

Unsere Magnetflusssonden sind mit hochgesättigtem Magnetfluss optimiert. Auswechselbare Verschleißringe verbessern die Verschleißbeständgkeit. Diese Sonden sind ideal zum Prüfen von Kühlluftrohren (mit Aluminiumrippen) und zum Prüfen von Rissen in Umfangsrichtung.

Features

  • Superior high-saturation optimized magnetic design.
  • Improved wear resistance and changeable wear rings.
  • Can detect outside volumetric defects.
  • Suitable for air-finned coolers.

Faster is better - Available for shortest delivery times

The probes listed below are regularly stocked for quick delivery. If the probe you require is not indicated, consult the "Alternate probe diameter" column in the Tube Inspection Probe Catalog to find an alternate probe diameter.

Part ID Item Number Diameter
mm in.
TFB-120-N20 U8280231 12 0.472
TFB-132-N20 U8280135 13.2 0.520
TFB-170-N20 U8280137 17 0.669
TFB-179-N20 U8280111 17.9 0.705
TFB-187-N20 U8280246 18.7 0.736
TFB-198-N20 U8280361 19.8 0.780
TFB-242-N20 U8280099 24.2 0.953

Standard/Custom Probes (Made to Order)

Use the nomenclature and the chart below to configure your part number.

Chart TFB

Probe Type Probe Diameter (use mm in part ID) Cable Length
Part Number Diameter mm** in.**
TFB: Magnetic flux leakage probe 120* 12.0 0.472 20 m (65 ft)
30 m (100 ft)
132* 13.2 0.520
161* 16.1 0.634
170* 17.0 0.669
179 17.9 0.705
187 18.7 0.736
198 19.8 0.780
229 22.9 0.902
242 24.2 0.953
283 28.3 1.114
296 29.6 1.165

* Smaller-diameter probes have less sentitivity to external defects, because the probe core section is much smaller than the tube section. However, the sensitivity to internal defects is still very high.

** These probes have an overall diameter that is slightly larger than the part number reference.

MFL Probe Selection Based on Tube Size

High-Saturation MFL Probe (TFB Model) Selection Guide for Common Carbon Steel Tube Sizes

Warning: If your tubes are dirty, a smaller probe might be required for the inspection. Olympus is not responsible if you select a probe that is not compatible with your application. If you require assistance, please contact an Olympus representative.

Example: For a one-inch tube with a wall thickness of 2.41 mm, the required probe would be TFB-187-N20. This probe has an overall diameter of 19.4 mm and changeable hardened steel half-rings.

Probe ID Diameter - mm (in.)
Tube Dimensions 12.0 (0.472) 13.2 (0.520) 16.1 (0.634) 17.0 (0.669) 17.9 (0.705) 18.7 (0.736) 19.8 (0.780) 22.9 (0.902) 24.2 (0.953) 28.3 (1.114) 29.6 (1.165)
OD
mm (in.)
BWG WT
mm (in.)
Overall Diameter (including wear system) - mm (in.)
12.5
to 12.8 (0.49 to 0.50)
13.7
to 14.0 (0.54 to 0.55)
16.6
to 16.9 (0.65 to 0.66)
18
(0.71)
18.7
(0.73)
19.4
(0.77)
20.5
(0.81)
23.8
(0.94)
25.1
(0.99)
29.2
(1.15)
30.5
(1.20)
19 (0.75) 16 1.65 (0.065)
14 2.11 (0.083)
13 2.41 (0.095)
12 2.77 (0.109)
25.4 (1.0) 16 1.65 (0.065)
15 1.83 (0.072)
14 2.11 (0.083)
13 2.41 (0.095)
12 2.77 (0.109)
11 3.05 (0.12)
10 3.40 (0.134)
9 3.76 (0.148)
31.75 (1.25) 13 2.41 (0.095)
12 2.77 (0.109)
11 3.05 (0.12)
10 3.40 (0.134)
38.1 (1.5) 12 2.77 (0.109)
11 3.05 (0.12)
10 3.40 (0.134)
9 3.76 (0.148)
Wear System Carbide beads (fixed) Hardened steel half-rings (changeable)