Inspection & Measurement Systems

Ultraschallprüfgeräte

Probes for Sub-Surface Corrosion and Crack Detection

Wirbelstrom-Array-Sensoren zur Prüfung von Korrosion und Rissen unter der Oberfläche von elektrisch leitendem Material, z. B. zur Prüfung von Überlappstößen an Flugzeugblechen aus Aluminium, von Korrosion zwischen Aluminiumblechen mit Überlappstoß und zur Korrosionserkennung unter dicken Aluminium-Überlappstößen (Schicht 3 und 4). Darüberhinaus besitzen diese Sensoren eine große Ankoppelfläche für schnelles Prüfen.

SAA-112-005-032 Probe Specifications

Typical application
Corrosion detection under conductive material. For example, the inspection of lap joints on aluminum airplane skins (layers 1 and 2); lap-joint inspection for corrosion detection between aluminum sheets.

Probe specifications
Probe coverage: 112 mm (4.4 in.)
Probe resolution: 3.5 mm (0.138 in.)
Frequency range: 1 kHz to 25 kHz
Number of elements: 32
Cable length: 3 m (10 ft)
Operation mode: Transmit-receive. Orientation at about 30°.
Penetration in aluminum: 1 mm to 3 mm (0.040 in. to 0.120 in.)
Detection capability: 5 % corrosion under 2 mm (0.080 in.) with a diameter of 6 mm (0.25 in.). 10 % corrosion under 3 mm (0.120 in.) with a diameter of 6 mm (0.25 in.).

SAA-056-005-016 Probe Specifications

Typical application
Corrosion detection under conductive material. For example, the inspection of aluminum lap joints, and airplane skins.

Probe specifications
Probe coverage: 56 mm (2.2 in.)
Probe resolution: 3.5 mm (0.138 in.)
Frequency range: 1 kHz to 25 kHz
Number of elements: 16
Cable length: 3 m (10 ft)
Operation mode: Transmit-receive. Orientation at about 30°.
Penetration in aluminum: 1 mm to 3 mm (0.040 in. to 0.120 in.)
Detection capability: 5 % corrosion under 2 mm (0.080 in.) with a diameter of 6 mm (0.25 in.). 10 % corrosion under 3 mm (0.120 in.) with a diameter of 6 mm (0.25 in.).

SAA-128-002-032 Probe Specifications

Typical application
Corrosion detection under thick aluminum lap joints (layers 3 and 4). As this probe is shielded, it offers better performance for deep corrosion under thick structures. In addition, this probe offers a larger footprint for rapid scanning.

Probe specifications
Probe coverage: 128 mm (5.04 in.)
Probe resolution: 4 mm (0.160 in.)
Frequency range: 0.4 kHz to 10 kHz
Number of elements: 32
Cable length: 3 m (10 ft)
Operation mode: Transmit-receive. Orientation at about 30°.
Penetration in aluminum: 3 mm to 6 mm (0.120 in. to 0.240 in.)
Detection capability: 10 % corrosion under 5 mm (0.200 in.) with a diameter of 12.5 mm (0.5 in.).

SCA-128-002-032 Probe Specifications

Used for the Gulfstream application as per NDT Manual references CB137 and CB188.
Probe specifications are identical to SAA-128-002-032.

SAA-064-002-032 Probe Specifications


Typical application
Corrosion detection under thick aluminum lap joints (layers 3 and 4). As this probe is shielded, it offers better performance for deep corrosion under thick structures. In addition, this probe offers a smaller footprint if access is restricted.

Probe specifications
Probe coverage: 64 mm (2.5 in.)
Probe resolution: 4 mm (0.160 in.)
Frequency range: 1.0 kHz to 20 kHz
Number of elements: 32
Cable length: 3 m (10 ft)
Operation mode: Transmit/receive. Orientation at about 30°.
Penetration in aluminum: 3.0 mm to 6.0 mm (0.120 in. to 0.240 in.)
Detection capability: 10 % corrosion under 5 mm (0.200 in.) with a diameter of 12.5 mm (0.5 in.)

SAA-064-002-016 Probe Specifications

Typical application
Corrosion detection under thick aluminum lap joints (layers 3 and 4). As this probe is shielded, it offers better performance for deep corrosion in thick structures. In addition, this probe offers a smaller footprint if access is restricted.

Probe specifications
Probe coverage: 64 mm (2.5 in.)
Probe resolution: 4 mm (0.160 in.)
Frequency range: 0.4 kHz to 10 kHz
Number of elements: 16
Cable length: 3 m (10 ft)
Operation mode: Transmit-receive. Orientation at about 30°.
Penetration in aluminum: 3 mm to 6 mm (0.120 in. to 0.240 in.)
Detection capability: 10 % corrosion under 5 mm (0.200 in.) with a diameter of 12.5 mm (0.5 in.).

SAB-067-005-032 Probe Specifications

Typical application
Corrosion and crack detection under conductive material. Can be used for lap-joint inspection (second layer crack and corrosion) and for doubler edge inspection (as per Boeing 737 Service Bulletin 53-30-25, part 6).

Probe specifications
Probe coverage: 67 mm (2.64 in.)
Probe resolution: 2.1 mm (0.082 in.)
Frequency range: 1 kHz to 25 kHz
Number of elements: 32
Cable length: 3 m (10 ft)
Operation mode: Transmit-receive on two rows and at about 30° orientation.
Penetration in aluminum: 1 mm to 3.5 mm (0.040 in. to 0.140 in.)
Detection capability: 3.8 mm (0.150 in.) long second layer crack at fastener. The first layer can have a thickness of up to 2 mm (0.080 in.) of aluminum, 5 % corrosion under 2 mm (0.080 in.) with a diameter of 6 mm (0.25 in.), 10 % corrosion under 3 mm (0.120 in.) with a diameter of 6 mm (0.25 in.).

SDBR-021-002-016 Probe Specifications

Typical application
Subsurface crack detection at fastener with a deep penetration in aluminum.

Probe specifications
Probe coverage: 21 mm (0.827 in.)
Probe resolution: 1.3 mm (0.052 in.)
Frequency range: 0.2 kHz to 10 kHz
Number of elements: 16
Cable length: 3 m (10 ft)
Operation mode: Differential transmit-receive using a large axial field (LAFEC)
Penetration in aluminum: Up to 6 mm
Detection capability: 3 mm (0.120 in.) long second and third layer crack at fastener.

SDCR-021-002-016 Probe Specifications

Typical application
Subsurface crack detection at fastener with a deep penetration in aluminum. In many cases, this probe provides simpler signal interpretation.

Probe specifications
Probe coverage: 21 mm (0.827 in.)
Probe resolution: 1.3 mm (0.052 in.)
Frequency range: 0.2 kHz to 10 kHz
Number of elements: 16
Cable length: 3 m (10 ft)
Operation mode: Absolute transmit-receive using a large axial field (LAFEC)
Penetration in aluminum: Up to 6 mm
Detection capability: 3 mm (0.120 in.) long second and third layer crack at fastener.