Eddy Current Examination of Gerth Gear
Forum Home  / Eddy Current and Eddy Current Array  / Applications
Author
Post
Joined: 11 Nov 2007
Posts: 4
Location:
 
Posted on So Nov 11, 2007 02:04   Post Subject: Eddy Current Examination of Gerth Gear
I would be interested in learning more about the examination of girth gear with eddy current method, the type of probes and equipment use to inspect large diameter gear. I been surfing the net to try to get information but nothing that I look at give me the information that I need. MT has been the prefer method for many years but it appears that some operator of large gear are asking to have eddy current examination perform in lieu of MT. Thanks
Joined: 09 Okt 2007
Posts: 8
Location:
 
Posted on So Nov 11, 2007 05:14   Post Subject: RE: Eddy Current Examination of Gerth Gear
Daniel - we have been involved with a Canadian company who is using Eddy Current Array probes for the inspection of large industrial gear teeth in lieu of penetrant and magnetic inspection. For this inspcetion we maufacture an array probe to suit the geometry of the gear tooth and the whole tooth is inspcted in a single pass. This particular customer is using the MS5800 and Multiview software, however, this inspection could be carried out using the Omniscan also. If this sounds like what you may be looking for, I can be contacted on email at aaron.greenbank@olympusndt for further information. I hope this helps.
Joined: 11 Nov 2007
Posts: 4
Location:
 
Posted on Sa Nov 17, 2007 03:35   Post Subject: RE: Eddy Current Examination of Gerth Gear
Aaron Greenbank wrote:
Daniel - we have been involved with a Canadian company who is using Eddy Current Array probes for the inspection of large industrial gear teeth in lieu of penetrant and magnetic inspection. For this inspcetion we maufacture an array probe to suit the geometry of the gear tooth and the whole tooth is inspcted in a single pass. This particular customer is using the MS5800 and Multiview software, however, this inspection could be carried out using the Omniscan also. If this sounds like what you may be looking for, I can be contacted on email at aaron.greenbank@olympusndt for further information. I hope this helps.


Could you give me a call at the Office on Monday November 19, 2007 604-275-3800
Joined: 09 Okt 2007
Posts: 8
Location:
 
Posted on So Nov 18, 2007 01:05   Post Subject: RE: Eddy Current Examination of Gerth Gear
Daniel,

Yes the OMNISCAN can be used for this and the Module is simply changed on the unit. I will give you a call on Monday as requested, we can discuss the application and costs associated then. Can you tell me what time zone you are in? I will be on Pacific time on Monday.

Aaron




Daniel wrote:
Thanks to provide some information regarding the inspection of large diameter girth gear. So an Omniscan can be used for that purpose. We have an ultrasonic phase array system, is the eddy current an added module and at what cost? As for the probes each gear is different so each time a gear is inspected a new probe must be purchase and again what is the cost of an eddy current probe array cost?
Please give me a call at
Joined: 11 Nov 2007
Posts: 4
Location:
 
Posted on Di Nov 20, 2007 02:49   Post Subject: RE: Eddy Current Examination of Gerth Gear
We are in Vancouver time which is three hours beyond Quebec city