Ultrasonic thickness gauging is not just limited to materials at normal (ambient) temperatures. The thickness of a part can be measured even when the surface temperature approaches 900 deg F (500 deg C). In metals, particularly, there may be circumstances when the thickness of the part needs to be measured before the part can be cooled down.

Ultrasonic testing has the advantage - just as at normal temperatures - that thickness measurements can be taken from one side of the hot part. Ultrasonics may be the preferred method of measurement even when both sides of the hot metal part are accessible. The reason is that ultrasonic thickness measurements can be made instantly and with very brief contact with the hot surface.

For the best calibrated accuracy, the effect of the higher temperature on the velocity of sound must be taken into account. Although change in sound velocity with temperature is much less in metals than in plastics, significant errors in measured thickness can result if sound velocity is not corrected.

Equipment: A major reason to classify hot metals separately is that when the temperature of a surface exceeds 120 deg F (50 deg C), Microscan contact transducers cannot be used because they will be damaged by thermal expansion effects. Consequently, gauges that exclusively utilize contact transducers cannot be used for making thickness measurements on hot surfaces.

We recommends the Model 35DL, which can be used with delay line transducers or immersion transducers. On hot surfaces delay line transducers must be used with selected High Temperature delay lines.
The thickness of hot corroded metal parts or parts with rough surfaces should be measured with the Model 38DL PLUS and a D790 or D791 dual transducer. The 38DL PLUS is a sophisticated multipurpose gage with internal data loggers and waveform displays that have practical features to provide excellent thickness measurement reliability on hot corroded metal pipes or tanks. For less challenging applications, the compact MG2 series of gages can also be used.

この用途に使用される製品

35DL

Das 35DL im Taschenformat ist ein Präzisionshanddickenmesser. Misst Metall, Kunststoff, Gummi, Glas und Verbundwerkstoffe mit Einzelschwingermesskopf. Dieselben Funktionen wie das Modell 35, aber mit eingebautem Messdatenspeicher.

38DL PLUS

Das 38DL PLUS ist ein hochentwickelter Ultraschalldickenmesser. Misst mit Sender-Empfängerschallkopf innere Korrosion; besitzt THRU-COAT und Echo-Echo-Funktion. Misst mit Einschwingermessköpfen dünne, sehr dicke oder mehrschichtige Stoffe sehr genau.

MG2

Der MG2 Ultraschalldickenmesser ist ein Handgerät, das mit Sender-Empfängermessköpfen Korrosion misst. Es besitzt viele Grundfunktionen, wie den Min/Max-Modus, mit dem Mindestdicken schnell aufgerufen werden (20 Messwerten pro Sekunde), den Einfriermodus, der augenblicklich kritische Dicken erfasst und den Nullpunktausgleich.