In cases where the test must be performed from the high impedance side of the joint, the ringdown technique described in this application note is often the best approach. This involves observing a series of multiple reflections from the boundary and looking for a difference in the rate at which the amplitude of successive echoes, or the ringdown envelope, changes between bond and disbond conditions. As the sound wave reverberates in the metal or other high impedance material,
the amplitude change is multiplied at each bounce, so for example a hard-to-see 5% amplitude drop between disbond and bond conditions at the first echo becomes a 25% drop at the fifth echo and a 50% drop at the tenth echo. While the change in a single echo may be small, the collective change across a series of multiple echoes will be much larger and easier to identify. In a typical joint, bond and disbond conditions will each produce their own distinctive ringdown pattern.
Set gain such that the first backwall echo is at full screen height. In the waveform below, the first peak is the delay line interface echo and the subsequent peaks are multiple echoes from a 0.1" (2.5 mm) unbonded steel standard. Because the metal is air-backed, the multiple echoes diminish at a relatively slow rate.
When using instruments that incorporate Distance Amplitude Correction (DAC) software, it will often be helpful to use the DAC function to draw the ringdown profile of a properly bonded part on the screen. That DAC curve may then be used to quickly identify absence of bonding, which will be indicated by a series of peaks that rise above the line as seen below. Additionally, instrument alarms may be set to trigger on echoes that rise above the curve to further identify suspect
bond conditions.
|
Das EPOCH 1000 ist ein hochenwickeltes Prüfgerät für konventionellen Ultraschall, das in einem zugelassenen Olympus Kundendienststelle mit der Phased-Array-Darstellung aufgebessert werden kann. Seine wichtigesten Merkmale sind Konformität mit EN12668-1, 37 einstellbare Digitalfilter am Empfänger und Impulsfolgefrequenz von 6 kHz für schnelle Prüfung.
Das EPOCH 600 ist ein Ultraschallhandprüfgerät der mittleren Klasse. Es wiegt nur 1,68 kg, sein horizontales Gehäuse widersteht sehr schwierigen Prüfumgebungen. Entspricht EN12668-1; weist unter anderem Funktionen wie den einstellbaren PerfectSquareTM Rechteckimpuls von 400 V und Digitalfilter auf, die das Signal-Rauschverhältnis verbessern.
Das EPOCH XT ist ein hochentwickeltes tragbares Ultraschallprüfgerät mit vielen Standardfunktionen wie einstellbarem Rechteckimpuls, einstellbarem Schmalband- und Breitbanddigitalfilter, Verstärkungsbereich von 0 bis 110 dB, Spitzenwertspeicher und Halten des Spitzenwertes, einstellbarer IFF, 0,01 mm.Copyright 2011 OLYMPUS CORPORATION, Alle Rechte vorbehalten. Nutzungsbedingungen | Datenschutzerklärung