Analysis of Glass MaterialFocus
Based on proven X-ray Fluorescence (XRF) technology, the Olympus Innov-X handheld XRF can be specially calibrated for glass-ceramic analysis. The Glass-Ceramic standard Analytical mode will allow the user to easily detect glass-ceramic (GC) or leaded glass. Optionally, this technology offers the powerful FastID mode which allows the user to identify the specific type or manufacturer of a glass-ceramic sample via cross-referencing to an extensive and unique database. |
Within seconds - detect leaded glass and glass-ceramic in a recycled glass cullet; ID glass by type or manufacturer. |
Detect and Identify:
Handheld XRF Features & Benefits
|
Hands free test stand to easily test small or oddly shaped samples
| Basic Specifications: | Handheld XRF-GC |
| Weight: | 2.625 lbs. (base wt.) 3.375 lbs (1.6 kg) with batteries |
| Excitation Source: | X-ray tube, Ag anode, 10-40 kV, 10 -5- µA, up to 5 filter positions |
| Detector: | Si PiN diode detector |
| Operating Environment: | Temperature: -10°C to 45°C, Humidity: 10% to 90% RH, non-condensing, Altitude Rating: 2,000 meters |
| Test Surface Temperature Range: | up to 900°F |
| Operation: | Trigger or Start/Stop Icon. One touch trigger or "deadman" trigger option. Optional control from external PC |
| Power: | Rechargeable Li-ion batteries (charger included). Powers analyzer and iPAQ simultaneously. AC Adapter optional |
| Battery Life: | 6-8 hours (typical duty cycle) |
| Analytical Analysis Package: | Standard package includes 21 elements. Customer may specify 4 additional, or use multiple suites of 25 elements each |
| Display Screen: | Color, high resolution touchscreen. Variable brightness provides easy viewing in all ambient lighting conditions |
| Data Display: | Concentrations displayed in percent. Spectral display with peak zoom and identification |
| Data Storage/Memory: | 128 MB standard memory. 20,000 test results with spectra, upgrade to >100,000 with optional 1 GB flash card |
| Processor/RAM: | Intel 400 MHz StrongArm processor or higher |
| Operating System: | Microsoft Windows CE (portable system) or Windows (PC-based). Software Modes: Analytical |
| Housing: | Reinforced LEXAN™ housing |
| Specifications subject to change without notice | |
| Options/Accessories | |
| FastID Mode: | Cross-references sample to exclusive glass library to ID the specific type and/or manufacturer of Glass Ceramic. |
| Test Stand: | Hands free test stand to easily test small or oddly shaped samples |
High Volume Glass SortingIn addition to portable solutions, Innov-X introduces the Redwave X-STREAM Glass; a unique automated system to effectively separate heat resistant and leaded glass from recycled glass cullet.This new system combines BT-Wolfgang Binder's proven REDWAVE optical sorting technology with Olympus Innov-X's high volume X-STREAM Glass sorting system. The result of this cooperation is a novel, high-volume system that analyzes glass by highly specific material chemistry. |
Die DELTA Handgeräte zur Röntgenfluoreszenzanalyse für Verbrauchersicherheit und RoHS-Übereinstimmung prüfen große Mengen von Verbraucher- und Elektronikprodukten überall und jederzeit. Die Konformitätsprüfung des Gehalts an Pb, Cd, Hg, Br und anderer Stoffe mit den Normen ASTM Method F2617-08, HR4040, CPSC, CPSIA und anderen, ist einfach schnell und zerstörungsfrei.
Das DELTA Handgerät zur Röntgenfluoreszenzanalyse von Schrott idenfiziert die meisten Legierungen und Reinmetalle zuverlässig in 1-2 Sekunden. Es ist dauerhaft gebaut und widersteht der rauesten Prüfumgebung. Sekundenschnelles, zuverlässiges Sortieren von Legierungen und Analyse einer breiten Palette von eisenhaltigen und nicht eisenhaltigen Materialien.
Das automatisierte Sortierungs- und Recycling-System X-STREAM mit Röntgenfluoreszenztechnik ist dafür programmiert, automatisch Stoffe anhand ihrer chemischen Zusammensetzung zu identifizieren und zu sortieren. Bringt das Recycling auf ein neues Niveau; genaues Sortieren von Schrottschredder, nicht ferritischen Metallen, Glas, Kunstoffen, Holz, Elektronikaltgeräten, Altfahrzeugen, Müllverstromung und mehr.Copyright 2011 OLYMPUS CORPORATION, Alle Rechte vorbehalten. Nutzungsbedingungen | Datenschutzerklärung