1 00:00:09,900 --> 00:00:11,233 Hi, I’m Ted Shields 2 00:00:11,233 --> 00:00:12,333 and I’m going to show you today 3 00:00:12,333 --> 00:00:15,566 just how easy it is to edit a grade specification 4 00:00:15,566 --> 00:00:18,266 in a grade library on the Vanta. 5 00:00:18,266 --> 00:00:20,366 You need to be in either Alloy or Alloy Plus 6 00:00:20,366 --> 00:00:21,433 because that’s where we are doing 7 00:00:21,433 --> 00:00:23,166 our grade identifications. 8 00:00:23,166 --> 00:00:24,900 Just go to the upper right and scroll down, 9 00:00:24,900 --> 00:00:26,900 that brings down your main menu tray. 10 00:00:26,900 --> 00:00:29,700 And then hit grade match. 11 00:00:29,700 --> 00:00:31,433 So we scroll down a little bit there 12 00:00:31,433 --> 00:00:33,466 to pick up our grade library setting. 13 00:00:33,466 --> 00:00:36,066 Select the grade library. 14 00:00:36,066 --> 00:00:37,900 And then use the pencil icon 15 00:00:37,900 --> 00:00:41,066 which just means that we’re going to edit. 16 00:00:41,066 --> 00:00:42,966 So we’ll edit one and a quarter chrome 17 00:00:42,966 --> 00:00:44,733 which is our top entry here. 18 00:00:44,733 --> 00:00:46,133 And we find a bunch of settings. 19 00:00:46,133 --> 00:00:48,500 The top setting is the Beam Flag. 20 00:00:48,500 --> 00:00:50,633 Beam Flag means that we try to do 21 00:00:50,633 --> 00:00:52,600 a grade match in the first beam. 22 00:00:52,600 --> 00:00:54,500 There are some grades that you only want 23 00:00:54,500 --> 00:00:57,366 to try to do a match in the second beam. 24 00:00:57,366 --> 00:01:00,100 The Smart Grade Flag is another setting 25 00:01:00,100 --> 00:01:01,466 that we’ll do a video on. 26 00:01:01,466 --> 00:01:03,833 The Smart Grade means that we end our analysis 27 00:01:03,833 --> 00:01:05,500 after the first beam when we can 28 00:01:05,500 --> 00:01:07,400 unambiguously identify the grade 29 00:01:07,400 --> 00:01:08,700 in that first beam. 30 00:01:08,700 --> 00:01:10,133 We’ve got our nominal base, 31 00:01:10,133 --> 00:01:11,566 one and a quarter chrome is iron. 32 00:01:11,566 --> 00:01:12,700 We’ve got a message. 33 00:01:12,700 --> 00:01:14,366 I’m going to go ahead and edit this. 34 00:01:14,366 --> 00:01:17,066 It’s got a couple of alternative names. 35 00:01:17,066 --> 00:01:21,300 I’m going to edit this to say high chrome. 36 00:01:21,300 --> 00:01:24,900 And then we’re going to go and edit the chrome entry. 37 00:01:24,900 --> 00:01:27,000 So just touch on the chrome line 38 00:01:27,000 --> 00:01:30,266 and then in where it says max let’s change the maximum 39 00:01:30,266 --> 00:01:33,800 let’s say to two just to pick a number. 40 00:01:33,800 --> 00:01:35,600 Hit update. 41 00:01:35,600 --> 00:01:37,800 And there, your grade library is updated, 42 00:01:37,800 --> 00:01:40,533 and those are the settings that we’ll be using moving forward. 43 00:01:40,533 --> 00:01:42,400 A couple of other things that you can do here, 44 00:01:42,400 --> 00:01:43,700 we have icons for, 45 00:01:43,700 --> 00:01:45,433 of course the trash can means to delete. 46 00:01:45,433 --> 00:01:47,533 Press it twice to have the delete be active. 47 00:01:47,533 --> 00:01:49,300 We don’t want to have an inadvertent touch 48 00:01:49,300 --> 00:01:51,666 accidentally delete something. 49 00:01:51,666 --> 00:01:53,166 If we move back out you also see 50 00:01:53,166 --> 00:01:54,566 we have a clone button. 51 00:01:54,566 --> 00:01:56,266 That lets you copy a grade 52 00:01:56,266 --> 00:02:00,200 or on the other page it lets you copy an entire grade library 53 00:02:00,200 --> 00:02:03,666 so that you can use that as a base to start from. 54 00:02:03,666 --> 00:02:05,966 Or if you wanted to enter a grade from scratch 55 00:02:05,966 --> 00:02:07,900 you can just hit the plus icon 56 00:02:07,900 --> 00:02:11,200 and that will add a new grade. 57 00:02:11,200 --> 00:02:12,566 So we come back here again 58 00:02:12,566 --> 00:02:14,733 we see the clone for the grade library. 59 00:02:14,733 --> 00:02:17,966 And then back to the grade match page. 60 00:02:17,966 --> 00:02:20,666 Scroll up to put away your main menu. 61 00:02:20,666 --> 00:02:23,666 So we’re back at the analysis page, 62 00:02:23,666 --> 00:02:25,100 so let’s go ahead and take a test 63 00:02:25,100 --> 00:02:27,800 and make sure that our settings are all in here. 64 00:02:27,800 --> 00:02:29,033 And we look and see, 65 00:02:29,033 --> 00:02:31,333 yeah we’ve got our edited grade message. 66 00:02:31,333 --> 00:02:34,033 We also have the edited maximum for chrome. 67 00:02:34,033 --> 00:02:35,833 And so it’s just that simple to go ahead 68 00:02:35,833 --> 00:02:37,800 and edit the grade specifications 69 00:02:37,800 --> 00:02:39,833 in a grade library on the Vanta. 70 00:02:39,833 --> 00:02:42,033 Thanks for watching, take care.