Our Altas European Standard Transducers are available in Dual Element, Angle Beam, Contact, and Protected Face styles designed to meet inspection criteria referenced throughout Europe and the rest of the world. Our Altas transducers are available in metric unit element diameters and common frequencies, such as 1, 2, 4, 5, and 6 MHz.
Dual Element Transducers

DL2R-7X18 (left image), DL4R-3.5X10 (right image)
Freq
MHz | Nominal Element Size
mm | Transducer Part # | Focus
in Steel
mm | Typical Bandwidth
(%) | Connector | Connector
Location | Outline # |
| 2 | 7 x 18 | DL2R-7X18 | 15 | 50 | LEMO 00 (2) | Right Angle | 2 |
| 7 x 18 | DL2R-7X18-0 | 30 | 50 | LEMO 00 (2) | Right Angle | 2 |
| 11 | DL2R-11 | 8 | 48 | LEMO 00 (2) | Right Angle | 1 |
| 4 | 3.5 x 10 | DL4R-3.5X10 | 10 | 45 | LEMO 00 (2) | Right Angle | 1 |
| 6 x 20 | DL4R-6X20 | 12 | 48 | LEMO 00 (2) | Right Angle | 2 |
| 6 x 20 | DL4R-6X20-0 | 25 | 48 | LEMO 00 (2) | Right Angle | 2 |
DGS diagrams are included with all Dual Element Transducers.
 |
 |
| 2 |
1 |
Integral Angle Beam Transducers
Freq.
MHz | Nominal Element Size mm | Angle
(°) | Near Field in steel mm | Transducer Part # | Typical Bandwidth | Connector (%) | Connector
Location | Outline # |
| 1 | 20 x 22 | 45 | 45 | AM1R-20X22-45 | 55 | LEMO® 01 | Right Angle | 9 |
| 20 x 22 | 60 | 45 | AM1R-20X22-60 | 55 | LEMO 01 | Right Angle | 9 |
| 20 x 22 | 70 | 45 | AM1R-20X22-70 | 55 | LEMO 01 | Right Angle | 9 |
| 2 | 8 x 9 | 45 | 15 | AM2R-8X9-45 | 40 | LEMO 00 | Right Angle | 6 |
| 8 x 9 | 45 | 15 | AM2S-8X9-45 | 40 | LEMO 00 | Straight | 7 |
| 8 x 9 | 60 | 15 | AM2R-8X9-60 | 40 | LEMO 00 | Right Angle | 6 |
| 8 x 9 | 60 | 15 | AM2S-8X9-60 | 40 | LEMO 00 | Straight | 7 |
| 8 x 9 | 70 | 15 | AM2R-8X9-70 | 40 | LEMO 00 | Right Angle | 6 |
| 8 x 9 | 70 | 15 | AM2S-8X9-70 | 40 | LEMO 00 | Straight | 7 |
| 14 x 14 | 45 | 39 | AM2R-14X14-45 | 45 | LEMO 00 | Right Angle | 8 |
| 14 x 14 | 60 | 39 | AM2R-14X14-60 | 45 | LEMO 00 | Right Angle | 8 |
| 14 x 14 | 70 | 39 | AM2R-14X14-70 | 45 | LEMO 00 | Right Angle | 8 |
| 20 x 22 | 38 | 90 | AM2R-20X22-38 | 40 | LEMO 01 | Right Angle | 5 |
| 20 x 22 | 45 | 90 | AM2R-20X22-45 | 40 | LEMO 01 | Right Angle | 9 |
| 20 x 22 | 60 | 90 | AM2R-20X22-60 | 40 | LEMO 01 | Right Angle | 9 |
| 20 x 22 | 70 | 90 | AM2R-20X22-70 | 40 | LEMO 01 | Right Angle | 9 |
| 4 | 8 x 9 | 38 | 30 | AM4R-8X9-38 | 40 | LEMO 01 | Right Angle | 6 |
| 8 x 9 | 45 | 30 | AM4R-8X9-45 | 40 | LEMO 00 | Right Angle | 6 |
| 8 x 9 | 45 | 30 | AM4S-8X9-45 | 40 | LEMO 00 | Straight | 7 |
| 8 x 9 | 60 | 30 | AM4R-8X9-60 | 40 | LEMO 00 | Right Angle | 6 |
| 8 x 9 | 60 | 30 | AM4S-8X9-60 | 40 | LEMO 00 | Straight | 7 |
| 8 x 9 | 70 | 30 | AM4R-8X9-70 | 40 | LEMO 00 | Right Angle | 6 |
| 8 x 9 | 70 | 30 | AM4S-8X9-70 | 40 | LEMO 00 | Straight | 7 |
| 20 x 22 | 45 | 180 | AM4R-20X22-45 | 40 | LEMO 01 | Right Angle | 9 |
| 20 x 22 | 60 | 180 | AM4R-20X22-60 | 40 | LEMO 01 | Right Angle | 9 |
| 20 x 22 | 70 | 180 | AM4R-20X22-70 | 40 | LEMO 01 | Right Angle | 9 |
| 5 | 14 x 14 | 45 | 88 | AM5R-14X14-45 | 40 | LEMO 00 | Right Angle | 7 |
| 14 x 14 | 60 | 88 | AM5R-14X14-60 | 40 | LEMO 00 | Right Angle | 7 |
| 14 x 14 | 70 | 88 | AM5R-14X14-70 | 40 | LEMO 00 | Right Angle | 7 |
| 6 | 3 x 4 | 45 | N/A | AM6S-3X4-45 | 38 | Microdot® | Straight | 10 |
| 3 x 4 | 60 | N/A | AM6S-3X4-60 | 38 | Microdot | Straight | 10 |
| 3 x 4 | 70 | N/A | AM6S-3X4-70 | 38 | Microdot | Straight | 10 |
DGS diagrams are included with all Integral Angle Beam Transducers except AM6S-3x4-45, AM6S-3x4-60 and AM6S-3x4-45.
Contact Transducers

CN2R-24
Freq.
MHz | Nominal
Element
Size mm | Transducer Part # | Near
Field mm | Typical
Bandwidth (%) | Connector | Connector
Location | Outline # |
| 2 | 10 | CN2R-10 | 7.2 | 85 | LEMO® 00 | Right Angle | 3 |
| 24 | CN2R-24 | 45 | 85 | LEMO 00 | Right Angle | 4 |
| 4 | 10 | CN4R-10 | 15.6 | 85 | LEMO 00 | Right Angle | 3 |
| 24 | CN4R-24 | 91 | 85 | LEMO 00 | Right Angle | 4 |
| 5 | 5 | CN5R-5 | 5 | 60 | Microdot | Right Angle | 5 |
| 10 | 5 | CN10R-5 | 10 | 60 | Microdot | Right Angle | 5 |
DGS diagrams are currently not available for Contact Transducers.
Protected Face Transducers

PF2R-10 (left image), PF4R-24 (right image)
| Freq. MHz | Nominal Element Size mm | Transducer Part # | Near Field mm | Typical Bandwidth (%) | Connector | Connector
Location | Outline # |
| 1 | 24 | PF1R-24 | 23 | 45 | LEMO 1 | Right Angle | 12 |
| 24 | PF1S-24 | 23 | 45 | LEMO 1 | Straight | 11 |
| 2 | 10 | PF2R-10 | 7.2 | 45 | LEMO 00 | Right Angle | 13 |
| 24 | PF2R-24 | 45 | 45 | LEMO 1 | Right Angle | 12 |
| 24 | PF2S-24 | 45 | 45 | LEMO 1 | Straight | 11 |
| 4 | 10 | PF4R-10 | 15.6 | 35 | LEMO 00 | Right Angle | 13 |
| 24 | PF4R-24 | 91 | 30 | LEMO 1 | Right Angle | 12 |
| 24 | PF4S-24 | 91 | 30 | LEMO 1 | Straight | 11 |
DGS diagrams are included with all Protected Face Transducers.
Protective Membrane Accessories

PM-24-12 (left image), MRN-24 (right image)
| Description | Fits With Nominal Element Size | Part Number |
| mm | |
| Set of 12 Membranes | 10 | PM-10-12 |
| Set of 12 Membranes | 24 | PM-24-12 |
| Retaining Ring | 10 | MRN-10 |
| Retaining Ring | 24 | MRN-24 |

Also available is the