Braze Joint Testing

Application: Testing the integrity of metallic braze joints in metal tubing and other parts.

Background: Brazing is a common process for joining sections of small diameter metal tubing and certain other small metal parts such as electrical contacts. It bonds two pieces of metal by means of a metallic filler that is melted and then flowed into the space between them by capillary attraction. The process is similar to soldering. The filler metal, which is commonly an alloy of copper, silver, tin and/or zinc with a relatively low melting point, must fill the space between the two parts being joined, wet the surfaces, and fuse them when it cools and solidifies. If the braze metal does not flow properly or does not fuse, the integrity of the joint will be affected. This problem can usually be identified with an ultrasonic flaw detector.

Equipment: Most braze joints can be tested with any Olympus ultrasonic flaw detector, including the EPOCH LTC, EPOCH 600, EPOCH XT, and EPOCH 1000. Given the typical geometry of braze joints, small diameter contact or delay line transducers are usually used. The transducer should be selected with respect to the geometry of the specific joint being tested, but for typical small diameter tubing the V208-RM (20 MHz) and V260 Sonopen (15 MHz) transducers are most commonly recommended.

Procedure: Braze joints are typically tested by means of a straight beam test that monitors the amplitude of the echo from the inside surface of the outer metal part. In the case of a good braze joint at the test point, the metal-to-metal bond will return a relatively small reflection, while an air gap will return a much larger one. These levels are established in each case by setting up on samples representing know brazed and un-brazed conditions.

The example below represents typical echoes from a braze joint between 9.5 mm (.0375 in.) and 12.5 mm (0.5 in.) copper tubing that was tested with a V208-RM transducer and an Epoch XT flaw detector. The first waveform shows a reference echo from an un-brazed area of the outer tube, which has been marked with a gate and set to nearly full screen height. The second waveform shows the response from a properly brazed point, in which the echo in the gated region drops to a very low level. By observing the amplitude of the echo within the gate, the operator can determine the joint condition at each test point by comparing the echo amplitude to these reference levels.

A partial braze within the area of the sound beam will be represented by a mid-level echo. Note: it is important to remember that very small discontinuities such as pinholes whose size is a small fraction of the beam diameter will not be detected through this procedure.

unbrazed joint screen

Typical echo response from unbrazed point.

brazed joint screen

Typical echo response from brazed point.

Products used for this application

EPOCH 1000 Series

The EPOCH 1000 is an advanced conventional ultrasonic flaw detector that can be upgraded with phased array imaging at an authorized Olympus service center. Key features include: EN12668-1 compliant, 37 digital receiver filter selections, and 6 kHz pulse repetition rate for high speed scanning.

EPOCH 600NEW

The EPOCH 600 is mid-level, handheld ultrasonic flaw detector. Weighing only 1.68 kg (3.72 lb.), its horizontal case is built to withstand the rigors of very harsh environments. EN12668-1 plus features such as 400 V PerfectSquare tunable square wave pulser, digital filtering for enhanced signal-to-noise ratio.

EPOCH LTC

The EPOCH LTC is a mid-level, handheld ultrasonic flaw detector in a compact 2.12 lbs (0.96 kg) vertical case. It is a full-featured instrument with EN12668-1 compliance and a wide variety of standard features as well as specialized options to meet your inspection needs.

EPOCH XT

The EPOCH XT is an advanced, portable ultrasonic flaw detector offering many standard measurement features including a tunable square wave pulser, selectable narrow-band and broad-band digital filters, gain range from 0 to 110 dB, peak memory and peak hold, and adjustable PRF.

Inspection & Measurement Systems
English | 日本語 | français | 简体中文 | Deutsch | italiano | čeština | magyar | Tiểng Việt | Español | русский | polski | português | 한국어

Pokročilé NDT technologie

Defektoskopy

Integrované inspekční systémy